Method for spin etching sidewall spacers by acid vapor
AssigneeTaiwan Semiconductor Manufacturing Company, Ltd.
InventorsJiunn-Der Yang, Chaucer Chnug, Yuan-Chang Huang
Life of this patent
Estimating the term…
Loading patent…
AssigneeTaiwan Semiconductor Manufacturing Company, Ltd.
InventorsJiunn-Der Yang, Chaucer Chnug, Yuan-Chang Huang
Estimating the term…
A method forming sidewall spacers on a semiconductor substrate without using the conventional plasma etching method is disclosed. In the method, a semiconductor substrate that has a gate structure formed on a top surface is first provided, followed by the deposition of a dielectric material layer on top of the semiconductor substrate. The substrate is then rotated to a rotational speed of at least 50 rpm, and an acid vapor is flown onto the substrate until the sidewall spacers are formed. The dielectric material layer for forming the sidewall spacers may be SiO2, SiON or Si3N4. The acid vapor utilized may be formed from an acid of HF, H3PO4, H2SO4 or HCl. In a preferred embodiment, the semiconductor substrate may be rotated to a rotational speed between about 100 rpm and about 150 rpm for a time period between about 10 sec. and about 20 sec.
A method for forming sidewall spacers on a semiconductor substrate comprising the steps of:
A method for etching dielectric spacers on a silicon substrate without causing plasma damages to the silicon substrate comprising the steps of:
Dependencies are inferred from the claim text.