Etching method
AssigneeMatsushita Electric Industrial Co., Ltd.
InventorNobuhiro Jiwari
Life of this patent
Estimating the term…
Abstract
The etching method of the present invention for forming a hole having a high aspect ratio in a silicon oxide film formed on a substrate via a silicon nitride film includes the step of performing etching using an etching gas composed of a mixture of Ar gas, O2 gas, C5F8 gas and CH2F2 gas.
Claims11
An etching method for forming a hole having a high aspect ratio in a silicon oxide film formed on a substrate via a silicon nitride film, the method comprising the step of:
- performing etching using an etching gas composed of a mixture of Ar gas, O2 gas, C5F8 gas and CH2F2 gas.
An etching method for forming a hole having a high aspect ratio in a laminated film formed on a substrate via a silicon nitride film, the laminated film including a lower layer composed of an impurity-containing silicon oxide film and an upper layer composed of a substantially impurity-free silicon oxide film, the method comprising the steps of:
- performing first-stage etching for the upper layer using a first etching gas composed of a mixture of Ar gas, O2 gas and C5F8 gas in a relatively large mixing ratio of the O2 gas to the fluorocarbon gas;
- and
- performing second-stage etching for the lower layer using a second etching gas composed of a mixture of Ar gas, O2 gas, C5F8 gas and CH2F2 gas in a relatively small mixing ratio of the O2 gas to the fluorocarbon gas.
An etching method for forming a second hole having a high aspect ratio in a laminated film formed on a silicon nitride film defining a first hole formed on a substrate, the laminated film including a lower layer composed of an impurity-containing silicon oxide film and an upper layer composed of a substantially impurity-free silicon oxide film, the second hole being made integral with the first hole, the method comprising the steps of
- performing first-stage dry etching for the upper layer using a first etching gas composed of a mixture of Ar gas, O2 gas and C5F8 gas in a relatively large mixing ratio of the O2 gas to the fluorocarbon gas;
- performing second-stage dry etching for the lower layer using a second etching gas composed of a mixture of Ar gas, O2 gas, C5F8 gas and CH2F2 gas in a relatively small mixing ratio of the O2 gas to the fluorocarbon gas;
- and
- removing a residue of the lower layer in the first hole by wet etching.
Dependencies are inferred from the claim text.