Workpiece comprising a laminate to protect against an impact stress
AssigneeFachhochschule Muenster
InventorsJuergen Peterseim, Denis Knust, Gerald Beermann
Life of this patent
Estimating the term…
Abstract
A method for applying a protective layer to protect against an impact stress includes mixing a sealing alloy in a powder form with a binder and water to form a pasty compound, applying the pasty compound on a surface to be protected, drying the applied pasty compound, and heating the dried applied pasty compound to a temperature of at least 800° C.
Claims4
A workpiece comprising a laminate to protect against an impact stress, the laminate being applied by a method comprising:
- mixing a sealing alloy in a powder form with a binder and water to form a pasty compound;
- applying a first coating of the pasty compound on a surface to be protected;
- applying a layer of a solid material to the first coating of the applied pasty compound;
- applying a second coating of the pasty compound on a surface of the layer of the solid material so as to form a laminate which comprises at least two layers of the pasty material and at least one layer of the solid material, the at least one layer of the solid material being arranged between the two layers of the pasty compound;
- and
- heating the laminate to a temperature of at least 800° C.,
- wherein, the layer of the solid material is steel.
A workpiece comprising a laminate to protect against an impact stress, the laminate being applied by a method comprising:
- mixing a sealing alloy in a powder form with a binder and water to form a pasty compound;
- applying a first coating of the pasty compound on a surface to be protected;
- applying a layer of a solid material to the first coating of the applied pasty compound;
- applying a second coating of the pasty compound on a surface of the layer of the solid material so as to form a laminate which comprises at least two layers of the pasty material and at least one layer of the solid material, the at least one layer of the solid material being arranged between the two layers of the pasty compound;
- and
- heating the laminate to a temperature of at least 800° C.,
- wherein,
- the pasty compound comprises,
- about 50 to <100 wt.-% of the sealing alloy, the sealing alloy being a chromium-containing nickel-based alloy comprising 0-4 wt.-% boron, 0-4 wt.-% silicon, and 0-1 wt.-% iron,
- >0 to 40 wt.-% of a binder, the binder being an enamel selected from a fusion mixture of silicates, borates and fluorides and a metal selected from at least one of sodium, potassium, lead and aluminum, and
- >0 to <10 wt.-% water,
- the wt.-%'s of the sealing alloy, the binder and the water adding up to 100 wt.-%, and
- the layer of the solid material is steel.
Dependencies are inferred from the claim text.