Hydrothermal synthesis of bismuth germanium oxide
AssigneeSandia Corporation
InventorTimothy J. Boyle
Life of this patent
Estimating the term…
Abstract
A method for the hydrothermal synthesis of bismuth germanium oxide comprises dissolving a bismuth precursor (e.g., bismuth nitrate pentahydrate) and a germanium precursor (e.g., germanium dioxide) in water and heating the aqueous solution to an elevated reaction temperature for a length of time sufficient to produce the eulytite phase of bismuth germanium oxide (E-BGO) with high yield. The E-BGO produced can be used as a scintillator material. For example, the air stability and radioluminescence response suggest that the E-BGO can be employed for medical applications.
Claims15
A method for the hydrothermal synthesis of bismuth germanium oxide, comprising;
- dissolving a bismuth precursor and a germanium precursor in water to provide an aqueous solution, and
- heating the aqueous solution in a sealed digestion bomb to a reaction temperature in the range of 150 to 200° C. for a length of time sufficient to produce an eulytite phase of bismuth germanium oxide.
Dependencies are inferred from the claim text.