“No-bake” foundry mix with extended work time
AssigneeASK Chemicals GmbH
InventorsMichael R. Nocera, Gregory P. Sturtz, Jörg Kroker
Life of this patent
Estimating the term…
Loading patent…
AssigneeASK Chemicals GmbH
InventorsMichael R. Nocera, Gregory P. Sturtz, Jörg Kroker
Estimating the term…
A “no-bake” process allows the forming of larger metal castings, by providing longer work times, in the range of about 45 to about 60 minutes. This is achieved using a liquid curing catalyst that is a pyridine, substituted at the second or third position with a moiety having a molecular weight in the range of about 30 to about 100 mwu. Examples of the liquid curing catalyst include 2-ethanolpyridine, 3-chloropyridine and 2-methoxypyridine. When combined with a two-part polyurethane binder precursor and a foundry aggregate, the liquid curing catalyst provides not only the longer work time, but also a strip time that is less than about 167% of the work time, as measured from the point of activating the polyurethane precursors by mixing them in the presence of the curing catalyst.
A binder composition for a foundry mix, comprising:
A foundry mix, comprising:
Dependencies are inferred from the claim text.