Back to results
US 9,357,657 B2Granted
Lead-free solder alloy for printed circuit board assemblies for high-temperature environments
AssigneeHalliburton Energy Services, Inc.
InventorsAndrew Albert Hrametz, Alexander T. Duncan
Life of this patent
Estimating the term…
Abstract
A solder alloy suitable for high temperature environments, such as for example electronic systems used in an oil or gas well where the temperature may be in the region of 175° C., the solder alloy having a Silver weight % in the range of 3.5 to 7.0, a Copper weight % in the range of 1.0 to 4.0, and an Antimony weight % in the range of 1.0 to 3.0. Other embodiments are described and claimed.
Claims12
A well logging tool comprising:
- an electronic system, the electronic system including one or more solder joints formed from a premelted solid lead-free wire-form solder having a preliminary solid solder alloy composition consisting of:
- Silver;
- Copper;
- Antimony;
- and
- Tin;
- wherein the preliminary solid solder alloy composition has a weight % of the Silver in a range of 3.5 to 7.0, a weight % of the Copper in a range of 1.0 to 4.0, and a weight % of the Antimony in a range of 1.0 to 3.0.
4 more elements
A well logging tool comprising:
- an electronic system, the electronic system including one or more solder joints formed from a premelted solid lead-free wire-form solder having a preliminary solid solder alloy composition consisting of:
- Silver;
- Copper;
- Antimony;
- Zinc;
- and
- Tin;
- wherein the preliminary solid solder alloy composition has a weight % of the Silver in a range of 3.5 to 7.0, a weight % of the Copper in a range of 1.0 to 4.0, a weight % of the Antimony in a range of 1.0 to 3.0;
- and a weight % of the Zinc in a range of 0.1 to 1.0.
6 more elements
A well logging tool comprising:
- an electronic system, the electronic system including one or more solder joints formed from a premelted solid lead-free wire-form solder having a preliminary solid solder alloy composition comprising:
- Silver;
- Copper;
- Antimony;
- and
- Tin;
- wherein the solder alloy composition has a weight % of the Silver in a range of 3.5 to 7.0, a weight % of the Copper in a range of 1.0 to 4.0, a weight % of the Antimony in a range of 1.0 to 3.0, and the remainder Tin.
4 more elements
Dependencies are inferred from the claim text.