US 9,356,095 B2Granted
Vertical devices and methods of forming
AssigneeMicron Technology, Inc.
InventorsAndrea Filippini, Luca Ferrario, Marcello Mariani
Life of this patent
Estimating the term…
Abstract
Vertical devices and methods of forming the same are provided. One example method of forming a vertical device can include forming a trench in a semiconductor structure, and partially filling the trench with an insulator material. A dielectric material is formed over the insulator material. The dielectric material is modified into a modified dielectric material having an etch rate greater than an etch rate of the insulator material. The modified dielectric material is removed from the trench via a wet etch.
Claims20
A device, formed by:
- forming a first insulator material in a trench;
- forming a dielectric material in the trench over the first insulator material;
- modifying the dielectric material into a second insulator material having an etch rate equal to or greater than an etch rate of the first insulator material;
- and
- removing a portion of the first insulator material and completely removing the second insulator material to expose a portion of a sidewall of the trench.
2 more elements
A device, formed by:
- partially filling a trench formed in a semiconductor structure with a first insulator material to a controlled depth;
- forming a dielectric material over the first insulator material;
- modifying the dielectric material into a second insulator material having an etch rate equal to or greater than an etch rate of the first insulator material;
- and
- removing a portion of the first insulator material and completely removing the second insulator material to expose a portion of a sidewall of the trench.
2 more elements
A device, comprising:
- semiconductor pillars;
- and
- a gate structure formed between the semiconductor pillars according to a method comprising:
- forming a first insulator material between the semiconductor pillars, the first insulator material having a first wet etch rate;
- forming a dielectric material between the semiconductor pillars over the first insulator material;
- annealing the dielectric material into a second insulator material at a temperature that results in the second insulator material having a second wet etch rate equal to or greater than the first etch rate;
- wet etching the second insulator material and a portion of the first insulator from between the semiconductor pillars;
- and
- forming the gate structure adjacent sidewalls of the semiconductor pillars upon a remaining portion of the first insulator material,
- wherein the temperature of annealing is selected such that wet etching results in removal of the second insulator material and the portion of the first insulator material on sidewalls of the semiconductor pillars at approximately a same time.
7 more elements
Dependencies are inferred from the claim text.