A process for preparing a substrate of a metal selected from the group consisting of titanium, tantalum, titanium alloys and tantalum alloys, modified by anodic spark deposition (ASD) on the surface thereof of a microporous and nanoroughened layer of the oxide of the same metal, enriched with Ca, P, Si, Na and at least one metal selected from the group consisting of:
- Ag and Ga, wherein said process consists of the following steps:
- a) cleaning the metal substrate by immersing the substrate in an ultrasound tray containing acetone for a first period of time of from 3 to 5 minutes and distilled water for a second period of time of from 3 to 5 minutes
- b) subjecting the metal substrate to an anodic spark deposition (ASD) treatment in an aqueous solution comprising sodium silicate hydrate (Na2SiO3.2H2O), β-glycerophosphate(β-GP), calcium acetate hydrate (C4H6CaO4.2H2O), sodium hydroxide (NaOH), at least one compound selected from the group consisting of:
- elemental Ag nanoparticles, an Ag and a Ga salt
- c) cleaning the metal substrate with water by immersing the metal substrate coming from step b) in distilled water and finally drying the same.