Aluminum alloy material for use in thermal conduction application
AssigneeNippon Light Metal Company, Ltd.
InventorsHiroshi Horikawa, Masahiko Shioda
Life of this patent
Estimating the term…
Loading patent…
AssigneeNippon Light Metal Company, Ltd.
InventorsHiroshi Horikawa, Masahiko Shioda
Estimating the term…
An aluminum alloy material for use in thermal conduction to which improved castability has been imparted by silicon addition. It has improved thermal conductivity and improved strength. The material has a composition containing 7.5-12.5 mass % Si and 0.1-2.0 mass % Cu, the remainder being Al and unavoidable impurities, wherein the amount of copper in the state of a solid solution in the matrix phase is regulated to 0.3 mass % or smaller. The composition may further contain at least 0.3 mass % Fe and/or at least 0.1 mass % Mg, provided that the sum of (Fe content) and (content of Mg among the impurities)×2 is 1.0 mass % or smaller and the sum of (Cu content), (content of Mg among the impurities)×2.5, and (content of Zn among the impurities) is 2.0 mass % or smaller.
An aluminum alloy die cast for use in a thermal conduction application, wherein the aluminum alloy die cast consists of 10.0 to 12.5 mass % of Si, 0.5 to 1.2 mass % of Cu, less than 0.05 mass % of Mg as an impurity, less than 0.05 mass % of Ti as an impurity, and Al and unavoidable impurities as the remainder, wherein a total amount of the unavoidable impurities is 0.1 mass % or less and the solid solution content of Cu in the matrix phase is 0.3 mass % or less.
An aluminum alloy die cast for use in a thermal conduction application, wherein the aluminum alloy die cast consists of 10.0 to 12.5 mass % of Si, 0.5 to 1.2 mass % of Cu, 0.1 to less than 0.2 mass % of Mg, less than 0.05 mass % of Ti as an impurity, and Al and unavoidable impurities as the remainder, wherein a total amount of the unavoidable impurities is 0.1 mass % or less, the relationship among the Cu content, the Mg content and the content of Zn included as an unavoidable impurity is such that the total of (Cu content)+(Mg content) times 2.5+(Zn content) is less than 1.8 mass %, and the solid solution content of Cu in the matrix phase is 0.3 mass % or less.
An aluminum alloy die cast for use in a thermal conduction application, wherein the aluminum alloy die cast consists of 10.0 to 12.5 mass % of Si, 0.5 to 1.2 mass % of Cu, less than 0.05 mass % of Mg as an impurity, less than 0.05 mass % of Ti as an impurity, and Al and unavoidable impurities as the remainder, wherein a total amount of the unavoidable impurities is 0.1 mass % or less and the solid solution content of Cu in the matrix phase is 0.3 mass % or less, subject to an ageing treatment within the range of at 180-300° C. for 4-8 hours.
An aluminum alloy die cast for use in a thermal conduction application, wherein the aluminum alloy die cast consists of 10.0 to 12.5 mass % of Si, 0.5 to 1.2 mass % of Cu, 0.1 to less than 0.2 mass % of Mg, less than 0.05 mass % of Ti as an impurity, and Al and unavoidable impurities as the remainder, wherein a total amount of the unavoidable impurities is 0.1 mass % or less, the relationship among the Cu content, the Mg content and the content of Zn included as an unavoidable impurity is such that the total of (Cu content)+(Mg content) times 2.5+(Zn content) is less than 1.8 mass %, and the solid solution content of Cu in the matrix phase is 0.3 mass % or less, subject to an ageing treatment within the range of at 180-300° C. for 4-8 hours.
Dependencies are inferred from the claim text.