Abstract
Light to ultra-light cement compositions with modified rheological properties. The cement composition includes cement, hydrophobic nano-silica, at least one additive and a sufficient amount of water to make a cement slurry with high compressive strength, low porosity, low free water, and low fluid loss with a quick thickening time.
Claims20
A modified cement composition comprising cement, hydrophobic nano-silica, at least one additive and a sufficient amount of water to make a cement slurry.
A modified cement composition comprising cement, hydrophobic nano-silica, and at least one additive and water to make a cement slurry having a 24-hour compressive strength of about 4450 psi.
A modified cement composition comprising cement with a particle size of from about 10 μm to about 50μm, hydrophobic nano-silica with a surface area of from about 110 m2/g to about 260 m2/g, at least one additive with a particle size of from about 51 μm to about 370 μm, and a sufficient amount of water to make a cement slurry.