US 9,353,252 B2Granted
Soft polypropylene with improved optical properties
AssigneeBorealis AG
InventorsMarkus Gahleitner, Martina Sandholzer, Klaus Bernreitner
Life of this patent
Estimating the term…
Abstract
Polymer composition comprising a propylene copolymer and a styrenic based elastomer.
Claims13
Polymer composition comprising:
- (a) a propylene copolymer (A) having:
- (a1) a melt flow rate MFR2 (230° C.) measured according to ISO 1133 in the range of more than 2.0 to 15.0 g/10 min,
- (a2) a comonomer content in the range of more than 7.5 to 16.5 wt. %, and
- (a3) a xylene cold soluble content (XCS) determined according to ISO 16152 (25° C.) in the range of 25.0 to 55.0 wt. %, wherein,
- (a4) the comonomer content of xylene cold soluble (XCS) fraction of the propylene copolymer (A) is in the range of 14.0 to 30.0 wt. %, and
- (a5) an intrinsic viscosity (IV) of the xylene cold soluble (XCS) fraction of the propylene copolymer (A) is in the range of equal or more than 1.5 to equal or below 3.0 dl/g, wherein the intrinsic viscosity (IV) is determined according to DIN ISO 1628/1 (in Decalin at 135° C.), and
- (b) styrenic based elastomer(s) (B) having a styrene content in the range of 5 to equal or below 15 wt. %,
- wherein further the weight ratio of propylene copolymer (A) and the styrenic based elastomer(s) (B) [(A)/(B)] is in the range of 9/1 to 3/2.
5 more elements
A container, comprising a film, the film including a polymer composition, the polymer composition comprising:
- (a) a propylene copolymer (A) having:
- (a1) a melt flow rate MFR2 (230° C.) measured according to ISO 1133 in the range of more than 2.0 to 15.0 g/10 min,
- (a2) a comonomer content in the range of more than 7.5 to 16.5 wt. %, and
- (a3) a xylene cold soluble content (XCS) determined according to ISO 16152 (25° C.) in the range of 25.0 to 55.0 wt. %, wherein,
- (a4) the comonomer content of xylene cold soluble (XCS) fraction of the propylene copolymer (A) is in the range of 14.0 to 30.0 wt. %, and
- (a5) an intrinsic viscosity (IV) of the xylene cold soluble (XCS) fraction of the propylene copolymer (A) is in the range of equal or more than 1.5 to equal or below 3.0 dl/g, wherein the intrinsic viscosity (IV) is determined according to DIN ISO 1628/1 (in Decalin at 135° C.), and
- (b) styrenic based elastomer(s) (B) having a styrene content in the range of 5 to equal or below 15 wt. %,
- wherein further the weight ratio of propylene copolymer (A) and the styrenic based elastomer(s) (B) [(A)/(B)] is in the range of 9/1 to 3/2.
5 more elements