US 9,353,206 B2Granted
Polyethylene composition having high swell ratio
AssigneeBassel Polylefine GmbH
InventorsIakovos Vittorias, Jens Wiesecke, Bernd Lothar Marczinke, Gerhardus Meier, Ulf Schüller, Volker Dolle, Johannes-Friedrich Enderle, Dieter Lilge, Barbara Gall
Life of this patent
Estimating the term…
Abstract
Polyethylene composition with improved swell ratio and mechanical properties, particularly suited for preparing blow-moulded articles, said composition having the following features: 1) density from 0.952 to 0.960 g/cm3; 2) ratio MIF/MIP from 17 to 30; 3) Shear-Induced Crystallization Index SIC from 2.5 to 5.0.
Claims10
A manufactured article comprising a polyethylene composition having:
- 1) a density from 0.952 to 0.960 g/cm3, determined according to ISO 1183 at 23° C.;
- 2) a ratio MIF/MIP from 17 to 30 wherein the MIF is the melt flow index at 190° C. with a load of 21.60 kg, and the MIP is the melt flow index at 190° C. with a load of 5 kg, both determined according to ISO 1133;
- 3) a SIC Index from 2.5 to 5.0;
- wherein the SIC Index is the Shear-Induced Crystallization Index, determined according to the following relation:
- SIC Index=(tonset,SIC@1000×tonset,quiescent)/(HLMI*100)
- where tonset,SIC@1000 is measured in seconds and is the time required for a crystallization onset under shear rate of 1000 s−1, the tonset, quiescent is measured in seconds and is the crystallization onset time at temperature of 125° C. under no shear, determined in isothermal mode by differential scanning calorimetry;
- HLMI is the melt flow index determined at 190° C. with load of 21.6 kg, according to ISO 1133.
4 more elements
A process for preparing a polyethylene composition having:
- 1) a density from 0.952 to 0.960 g/cm3, determined according to ISO 1183 at 23° C.;
- 2) a ratio MIF/MIP from 17 to 30 wherein the MIF is the melt flow index at 190° C. with a load of 21.60 kg, and the MIP is the melt flow index at 190° C. with a load of 5 kg, both determined according to ISO 1133;
- 3) a SIC Index from 2.5 to 5.0;
- wherein the SIC Index is the Shear-Induced Crystallization Index, determined according to the following relation:
- SIC Index=(tonset,SIC@1000×tonset,quiescent)/(HLMI*100)
- where tonset,SIC@1000 is measured in seconds and is the time required for a crystallization onset under shear rate of 1000 s−1, the tonset, quiescent is measured in seconds and is the crystallization onset time at temperature of 125° C. under no shear, determined in isothermal mode by differential scanning calorimetry;
- HLMI is the melt flow index determined at 190° C. with a load of 21.6 kg, according to ISO 1133;
- and
- wherein all the polymerization steps are carried out in the presence of a Ziegler-Natta polymerization catalyst supported on MgCl2.
6 more elements