Process for sintering silicon carbide
OwnerDale Adamsinventor
Life of this patent
Estimating the term…
Abstract
A process for sintering silicon carbide is provided which includes the steps of providing a silicon carbide powder of silicon carbide granules; purifying the silicon carbide powder; subjecting the purified silicon carbide powder to a gel-casting process; removing the gel-cast part from the mold; drying the gel-cast part; obtaining a dried cast ceramic part (a green body) which is capable of green machining into a final desired shape; firing the green body in an oven at temperatures ranging from about 100° C. to about 1900° C. to remove or burn out any polymer remaining in the ceramic; and sintering the green body at temperatures ranging from about 1600° C. to less than about 2200° C.
Claims21
A process for sintering silicon carbide comprising:
- a) providing a silicon carbide powder of silicon carbide granules;
- b) purifying the silicon carbide powder by
- b. 1) washing the silicon carbide powder with a solution of hydrofluoric acid,
- b. 2) rinsing the silicon carbide powder in distilled water;
- and
- b. 3) drying the silicon carbide powder to obtain a pure silicon carbide powder, wherein granules which form the silicon carbide powder are substantially free of a silicon dioxide shell;
- and
- c) subjecting the purified silicon carbide powder to a gel-casting process comprising the following steps:
- c. 1) mixing the silicon carbide powder with water or a non-aqueous solvent, a dispersant, and gel-forming organic monomers to obtain a ceramic slurry;
- c. 2) exposing the ceramic slurry to a partial vacuum to remove air from the ceramic slurry;
- c. 3) adding a polymerization initiator to the ceramic slurry to commence a gel-forming chemical reaction;
- c. 4) pouring the ceramic slurry into a mold and casting the ceramic slurry into a desired workpiece shape;
- and
- c. 5) heating the mold in a curing oven or setting the mold with a catalyst;
- d) removing a gel-cast part from the mold;
- e) drying the gel-cast part to remove the water or the non-aqueous solvent and obtain a dried cast ceramic part;
- f) firing the dried cast ceramic part in an oven at temperatures ranging from about 100° C. to about 1600° C.;
- and,
- g) sintering the dried cast ceramic part at temperatures ranging from about 1600° C. to less than about 2200° C., wherein the dried cast ceramic part is sintered within a capped crucible of pressurized molten liquid, wherein the pressure is obtained by capping of the crucible and application of vibratory forces to the molten liquid.
Dependencies are inferred from the claim text.