US 9,352,976 B2Granted
Methods for preparing trimanganese tetroxide with low bet specific surface area, methods for controlling particle size of trimanganese tetroxide and trimanganese tetroxide product
AssigneeGuizhou Redstar Developing Co., Ltd.
InventorsZhiguang Jiang, Dong Hua, Zhengtao Liu, Kaiwen Zeng
Life of this patent
Estimating the term…
Abstract
The present invention provides methods for preparing trimanganese tetroxide with low BET specific surface area and methods for controlling particle size of trimanganese tetroxide and trimanganese tetroxide product.
Claims10
A method for preparing trimanganese tetroxide, comprising:
- (1) a process for purifying air comprising purifying air by spraying dilute aqueous ammonia;
- (2) a pretreatment of removing impurities from MnSO4 solution comprising adjusting pH value of the MnSO4 solution with a concentration in a range of 150˜200 g/L to 5.5-6.0, introducing H2S gas into the MnSO4 solution until pH value reaches 2.5-3.0, separating the mixture by solid-liquid separation to obtain a filtrate and a solid, purifying the filtrate by removing impurities with oxidization of H2O2, adjusting pH value of the filtrate to 5-6 with a base, and separating the obtained mixture by solid-liquid separation to obtain a filtrate and a solid, so as to obtain MnSO4 solution as filtrate for use;
- (3) a process for preparing seed crystal comprising cooling the MnSO4 solution obtained in the process (2) from MnSO4 solution to a temperature of less than 40° C., and introducing liquid NH3 into the cooled MnSO4 solution until pH value reaches 10.5-11.0, separating the mixture by solid-liquid separation to obtain a filtrate and a solid;
- washing the obtained solid, adding deionized water to the washed solid and forming a slurry, introducing the purified air obtained in the process (1) into the slurry, and oxidizing the slurry into Mn3O4;
- separating the mixture by solid-liquid separation to obtain filtrate and solid, so as to obtain Mn3O4 seed crystal as solid for use;
- and
- (4) a process for obtaining the final product by controlling oxidization comprising adding the MnSO4 solution obtained in the process (2) from MnSO4 solution into an oxidization reactor, adding Mn3O4 seed crystal obtained in the process for preparing seed crystal (3) according to the proportion of (0.012-0.040) kg of Mn3O4 seed crystal per cubic meter of the MnSO4 solution, adding the liquid ammonia, introducing the purified air obtained in the process for purifying air (1) into a reactor and turning on the recycle pump, controlling the temperature of the system in a range of 25±5° C., controlling pH value of the reaction system in a range of 6.5-7.5, which makes the MnSO4 solution circulate more than 6 times per hour so as to carry out circulatory oxidization reaction, not stopping the reaction until MnSO4 content of the reaction solution equal to or is less than 1.5 g/L, separating the mixture by solid-liquid separation to obtain a filtrate and a solid, washing and drying the solid to obtain Mn3O4 product.
4 more elements
Dependencies are inferred from the claim text.