Back to results
US 9,352,450 B1Granted
Methods of cleaning a polycrystalline diamond body and methods of forming polycrystalline diamond compacts
AssigneeUS Synthetic Corporation
InventorsMichael A. Vail, Paul D. Jones
Life of this patent
Estimating the term…
Abstract
Embodiments of the invention relate to methods of cleaning a leaching agent and/or leaching agent by-products from an at least partially leached polycrystalline diamond body, and methods of making a polycrystalline diamond compact using the same.
Claims20
A method of cleaning an at least partially leached polycrystalline diamond body, the method comprising:
- positioning the at least partially leached polycrystalline diamond body within a pressure vessel such that at least one surface of the at least partially leached polycrystalline diamond body is exposed to an environment inside of the pressure vessel and at least one surface is exposed to an environment outside of the pressure vessel;
- at least partially filling the pressure vessel with a removal agent;
- elevating a pressure of the removal agent in the pressure vessel relative to an ambient atmospheric pressure of the environment outside of the pressure vessel;
- and
- exposing the at least partially leached polycrystalline diamond body to the removal agent in the pressure vessel.
2 more elements
A method of cleaning an at least partially leached polycrystalline diamond body, the method comprising:
- positioning the at least partially leached polycrystalline diamond body within a pressure vessel such that at least one surface of the at least partially leached polycrystalline diamond body is exposed to an environment inside of the pressure vessel and at least one is surface exposed to an environment outside of the pressure vessel;
- at least partially filling the pressure vessel with a removal agent including at least one of a supercritical component, an aqueous component, a chelating component, or an organic component;
- elevating a pressure and a temperature of the removal agent in the pressure vessel relative to an ambient atmospheric pressure and temperature of the environment outside of the pressure vessel to induce a supercritical state in at least one component of the removal agent;
- and
- exposing the at least partially leached polycrystalline diamond body to the removal agent.
2 more elements
Dependencies are inferred from the claim text.