Processes for preparing pulp and paper
AssigneesNippon Paper Industries Co., Ltd., Aikawa Iron Works Co., Ltd.
InventorsShisei Goto, Takaharu Noda, Hiroki Ohtake, Tatsumi Hosaka
Life of this patent
Estimating the term…
Loading patent…
AssigneesNippon Paper Industries Co., Ltd., Aikawa Iron Works Co., Ltd.
InventorsShisei Goto, Takaharu Noda, Hiroki Ohtake, Tatsumi Hosaka
Estimating the term…
The purpose of the present invention is to provide technology for regenerating pulp having high quality with compact pulp regenerating equipment and less energy. In the pulp regenerating method of the present invention, pulp slurry containing 1.5 wt % or more of a solid component including waste paper pulp is separated into a long fiber fraction and a short fiber fraction by using an outward type slit screen including an opening portion having a slit width in the range of 0.1 mm to 0.3 mm. The solid component ratio of the long fiber fraction and the short fiber fraction is in the range from 10:90 to 60:40, and the difference in Canadian Standard Freeness of the long fiber fraction and the short fiber fraction is in the range of 100 ml to 300 ml.
A process for treating waste paper pulp, which process comprises fractionating a waste paper pulp slurry having a solids content of 2.2% by weight or more into a long fiber fraction and a short fiber fraction using an outward flow slit screen having openings with a slit width of 0.13 mm to 0.3 mm, wherein the solids content ratio of the long fiber fraction to the short fiber fraction is 10:90 to 60:40 and wherein the difference in Canadian standard freeness between the long fiber fraction and the short fiber fraction is 100 ml to 300 ml.
A process for preparing recycled waste paper pulp, which process comprises fractionating a waste paper pulp slurry having a solids content of 1.5% to 2.2% by weight or more containing waste paper pulp into a long fiber fraction and a short fiber fraction using an outward flow slit screen having openings with a slit width of 0.13 mm to 0.2 mm, wherein the solids content ratio of the long fiber fraction to the short fiber fraction is 10:90 to 60:40 and wherein the difference in Canadian standard freeness between the long fiber fraction and the short fiber fraction is 100 ml to 300 ml., subjecting the short fiber fraction to an ink detachment step at a solids content of 5% or less by contacting the short fiber fraction with cavitation bubbles and then an ink removal step.
A process for preparing paper comprising fractionating a waste paper pulp slurry having a solids content of 1.5% to 2.2% by weight or more containing waste paper pulp into a long fiber fraction and a short fiber fraction using an outward flow slit screen having openings with a slit width of 0.13 mm to 0.2 mm, wherein the solids content ratio of the long fiber fraction to the short fiber fraction is 10:90 to 60:40 and wherein the difference in Canadian standard freeness between the long fiber fraction and the short fiber fraction is 100 ml to 300 ml., subjecting the short fiber fraction to an ink detachment step at a solids content of 5% or less by contacting the short fiber fraction with cavitation bubbles to form a treated short fiber fraction, subjecting the treated short fiber fraction to an ink removal step to form a first short fiber fraction, mixing the long fiber pulp and the first short fiber fraction with raw materials used to prepare paper to form a mixture and forming the mixture into paper.
Dependencies are inferred from the claim text.