Back to results
US 8,278,548 B2Granted
Acrylic film and acrylic backsheet prepared therefrom
AssigneeRohm and Haas Company
InventorsHailan Guo, Matthieu Olivier Sonnati, Robert Lee Post, David Elmer Vietti
Life of this patent
Estimating the term…
Abstract
An acrylic film including from 70% to 99%, by weight based on the weight of the film, of a certain multi-stage acrylic polymer and from 1% to 20%, by weight based on the weight of the film, pigment is provided. Also provided is a method for forming the acrylic film, a backsheet for a photovoltaic array that includes the acrylic film and a polyester layer, and a method for forming the backsheet.
Claims3
A photovoltaic array backsheet comprising:
- an acrylic film comprising:
- a multi-stage acrylic polymer comprising
- from 10% to 75% by weight, based on the weight of said multi-stage polymer, first polymer comprising, as copolymerized units, from 0% to 20% by weight, based on the weight of said first polymer, C1-C6 alkyl methacrylate, said methacrylate having a homopolymer glass transition temperature (“Tg”) of from 60° C. to 120° C. and from 80% to 100% by weight, based on the weight of said first polymer, C1-C12 alkyl acrylate, said acrylate having a homopolymer Tg of lower than 10° C.;
- and
- from 25% to 90% by weight, based on the weight of said multi-stage polymer, second polymer formed in the presence of said first polymer comprising, as copolymerized units, from 50% to 100% by weight, based on the weight of said second polymer, C1-C6 alkyl methacrylate, said methacrylate having a homopolymer glass transition temperature (“Tg”) of from 60° C. to 120° C.;
- from 0% to 20% by weight, based on the weight of said second polymer, C1-C12 alkyl acrylate, said acrylate having a homopolymer Tg of lower than 10° C., and from 0% to 30% by weight, based on the weight of said second polymer, of a polymer having a homopolymer Tg of higher than 120° C.;
- and from 1% to 20%, by weight based on the weight of said film, pigment;
- and
- affixed thereto, a polyester layer.
6 more elements
A method for forming a photovoltaic array backsheet comprising:
- forming an acrylic film composition comprising:
- from 70% to 99%, by weight based on the weight of said film, multi-stage acrylic polymer comprising
- from 10% to 75% by weight, based on the weight of said multi-stage polymer, first polymer comprising, as copolymerized units, from 0% to 20% by weight, based on the weight of said first polymer, C1-C6 alkyl methacrylate, said methacrylate having a homopolymer glass transition temperature (“Tg”) of from 60° C. to 120° C. and from 80% to 100% by weight, based on the weight of said first polymer, C1-C12 alkyl acrylate, said acrylate having a homopolymer Tg of lower than 10° C.;
- and
- from 25% to 90% by weight, based on the weight of said multi-stage polymer, second polymer formed in the presence of said first polymer comprising, as copolymerized units, from 50% to 100% by weight, based on the weight of said second polymer, C1-C6 alkyl methacrylate, said methacrylate having a homopolymer glass transition temperature (“Tg”) of from 60° C. to 120° C.;
- from 0% to 20% by weight, based on the weight of said second polymer, C1-C12 alkyl acrylate, said acrylate having a homopolymer Tg of lower than 10° C., and from 0% to 30% by weight, based on the weight of said second polymer, of a polymer having a homopolymer Tg of higher than 120° C.;
- and from 1% to 20%, by weight based on the weight of said film, pigment;
- forming an acrylic film from said composition by calendering or cast film formation;
- and
- affixing thereto, a polyester layer.
7 more elements
Dependencies are inferred from the claim text.