Additives and lubricant formulations having improved antiwear properties
AssigneeAfton Chemical Corporation
InventorsMark T. Devlin, Kenneth J. Garelick, Naresh C. Mathur, Jeffrey M. Guevremont
Life of this patent
Estimating the term…
Loading patent…
AssigneeAfton Chemical Corporation
InventorsMark T. Devlin, Kenneth J. Garelick, Naresh C. Mathur, Jeffrey M. Guevremont
Estimating the term…
Lubricated surfaces, lubricant compositions for lubricating a surface, and methods for increasing antiwear properties in lubricants. The lubricated surface is provided by a lubricant composition including a base oil of lubricating viscosity, at least one metal salt of phosphorothioic acid, and an amount of at least one hydrocarbon soluble titanium compound effective to provide an increase in antiwear properties of the lubricant composition. A ratio of titanium metal to phosphorus in the antiwear agent ranges from about 0.3:1 to about 1.5:1.
A lubricated surface comprising a lubricant composition including a base oil of lubricating viscosity, at least one metal salt of phosphorothioic acid, and an amount of at least one hydrocarbon soluble titanium compound comprising a reaction product of a titanium alkoxide and a carboxylic acid selected from the group consisting of a non-linear carboxylic acid and a carboxylic acid having more than 22 up to 25 carbon atoms, said titanium compounds being effective to provide an increase in antiwear properties of the lubricant composition wherein a weight ratio of titanium metal provided by the hydrocarbon soluble titanium compound to phosphorus in the antiwear agent ranges from about 0.3:1 to about 1.5:1.
A vehicle having moving parts and containing a lubricant for lubricating the moving parts, the lubricant comprising an oil of lubricating viscosity, a friction modifier, and an antiwear agent comprising an amount of at least one hydrocarbon soluble titanium compound comprising a reaction product of a titanium alkoxide and a carboxylic acid selected from the group consisting of a non-linear carboxylic acid and a carboxylic acid having more than 22 up to 25 carbon atoms, and an amount of at least one metal salt of phosphorothioic acid, wherein a weight ratio of titanium metal provided by the hydrocarbon soluble titanium compound to phosphorus in the antiwear agent ranges from about 0.3:1 to about 1.5:1 and the antiwear agent provides a antiwear film thickness that is greater than a film thickness provided by the titanium compound or phosphorus compound alone.
A fully formulated lubricant composition comprising a base oil component of lubricating viscosity, and an antiwear agent comprising an amount of hydrocarbon soluble titanium-containing compound comprising a reaction product of a titanium alkoxide and a carboxylic acid selected from the group consisting of a non-linear carboxylic acid and a carboxylic acid having more than 22 up to 25 carbon atoms, and an amount of at least one metal salt of phosphorothioic acid, wherein a weight ratio of titanium metal provided by the hydrocarbon soluble titanium compound to phosphorus in the antiwear agent ranges from about 0.3:1 to about 1.5:1.
A method for increasing an antiwear film thickness adjacent to a lubricated surface, comprising contacting the surface with a lubricant composition comprising a base oil of lubricating viscosity and an amount of an antiwear agent comprising a hydrocarbon soluble titanium compound comprising a reaction product of a titanium alkoxide and a carboxylic acid selected from the group consisting of a non-linear carboxylic acid and a carboxylic acid having more than 22 up to 25 carbon atoms, and a metal salt of phosphorothioic acid, wherein the antiwear agent has a titanium metal to phosphorus ratio by weight that provides a synergistic increase in the antiwear film thickness compared to an antiwear film thickness provided by a lubricant composition containing only one of the titanium compound and the metal salt of phosphorothioic acid.
An additive concentrate for a lubricant composition comprising an antiwear agent including at least one metal salt of phosphorothioic acid, and an amount of at least one hydrocarbon soluble titanium compound comprising a reaction product of a titanium alkoxide and a carboxylic acid selected from the group consisting of a non-linear carboxylic acid and a carboxylic acid having more than 22 up to 25 carbon atoms, said titanium compounds being effective to provide an increase in antiwear properties of the lubricant composition, wherein a weight ratio of titanium metal provided by the hydrocarbon soluble titanium compound to phosphorus in the antiwear agent ranges from about 0.3:1 to about 1.5:1.
Dependencies are inferred from the claim text.