Abstract
A cracking catalyst contains a substantially inert core and an active shell, the active shell containing a zeolite catalyst and a matrix. The catalyst is formed by spray-drying a slurry containing water, substantially inert microspheres and a zeolite precursor and crystallizing zeolite in the active shell to create the cracking catalyst. Methods of using the cracking catalyst are also described.
Claims23
A fluidizable cracking catalyst, comprising:
- from about 5% to less than 50% by volume a substantially inert core comprising mullite;
- and
- from 50% to about 95% by volume of an active shell comprising a NaY zeolite catalyst and a matrix, wherein the NaY zeolite catalyst is crystallized in the active shell after a slurry containing microspheres of mullite, NaY zeolite precursor, and matrix precursor is spray-dried,
- wherein the cracking catalyst maintains at least about 45% of original NaY zeolite surface area through standardized steaming.
A method of making a fluidizable cracking catalyst with an active shell at least partially surrounding a substantially inert core containing mullite, comprising:
- forming a slurry by combining at least water, about 1 to about 70 parts by weight hydrous kaolin, from about 1 to about 70 parts by weight spinel-form calcined kaolin, from about 1 to about 70 parts by weight mullite kaolin, and from about 1 to about 70 parts by weight substantially inert core microspheres containing mullite, and a zeolite precursor;
- and
- spray drying the slurry to form particles containing the substantially inert core microspheres with an active shell at least partially surrounding the substantially inert core;
- and
- crystallizing zeolite in the active shell to create the fluidizable cracking catalyst.
A cracking process, comprising:
- contacting a hydrocarbon feedstream and a cracking catalyst comprising from about 5% to less than 50% by volume a substantially inert core containing mullite and from 50% to about 95% by volume of an active shell comprising a zeolite catalyst and a matrix in a reactor at a temperature from about 300 to about 800° C. to provide a cracked product,
- wherein the cracking catalyst is prepared by spray drying a slurry, comprising water, microspheres of the substantially inert core, a zeolite precursor, and a matrix precursor, and crystallizing the zeolite catalyst in the active shell.
Dependencies are inferred from the claim text.