US 8,278,001 B2Granted
Low-porosity anode diffusion media for high concentration direct methanol fuel cells and method of making
AssigneesPanasonic Corporation, The Penn State Research Foundation
InventorsSeung Hun Jung, Chao-Yang Wang, Takashi Akiyama
Life of this patent
Estimating the term…
Abstract
A direct oxidation fuel cell (DOFC) having a liquid fuel and an anode electrode configured to generate power. The anode electrode includes a gas diffusion layer (GDL) and a microporous layer, such that a decrease in the porosity of the GDL achieves an increase in the power density of the DOFC.
Claims10
A direct oxidation fuel cell (DOFC) comprising:
- an anode electrode configured to generate power, the anode electrode having a gas diffusion layer (GDL) loaded with at least one polymer and a microporous layer;
- wherein the GDL has a porosity such that it increases the power density of the DOFC,
- wherein said porosity is adjusted by adjusting the polymer content of the GDL and,
- wherein said porosity is selected based on at least one of the group consisting of:
- operating temperature of the DOFC and
- current density of the DOFC,
- wherein, the DOFC is configured to have at least one selected from the group consisting of:
- an operating temperature of about 50° C. and porosity of about 0.59%;
- an operating temperature of 70° C. and porosity of about 0.48%;
- a current density of about 300 mA/cm2 and porosity of about 0.53%;
- and a current density is 200 mA/cm2 and porosity is about 0.41%,
- wherein one of the at least one polymer is a fluorinated polymer, and
- wherein the GDL is loaded at between 30 wt % to 70 wt % with the at least one fluorinated polymer.
10 more elements
A method of making a direct oxidation fuel cell (DOFC) comprising:
- configuring an anode electrode comprising a gas diffusion layer (GDL) and a microporous layer (MPL),
- selecting at least one of:
- a operating temperature of the DOFC and
- a current density of the DOFC, and
- adjusting the porosity of the GDL based on the operating temperature of the DOFC or the current density of the DOFC by adjusting a fluorinated polymer content of the GDL, to achieve a porosity of the GDL such that it increases the power density of the DOFC,
- wherein, the DOFC is configured to have at least one selected from the group consisting of:
- an operating temperature of about 50° C. and porosity of about 0.59%;
- an operating temperature of 70° C. and porosity of about 0.48%;
- a current density of about 300 mA/cm2 and porosity of about 0.53%;
- and a current density is 200 mA/cm2 and porosity is about 0.41%, and
- wherein said GDL is loaded at 30 wt % to 70 wt % with the at least one fluorinated polymer.
8 more elements
A method of operating a direct oxidation fuel cell (DMFC) system, comprising steps of:
- (a) providing at least one fuel cell assembly including a cathode and an anode with an electrolyte positioned therebetween, said anode comprising a gas diffusion layer (GDL) including a microporous layer, said microporous layer comprising an electrically conductive material and a fluoropolymer, loading of said fluoropolymer in said microporous layer being in the range from about 30 to about 70 wt. %;
- b) supplying a concentrated solution of a liquid fuel and water to said anode;
- c) operating said at least one fuel cell assembly in at least one selected from the group consisting of:
- at a temperature of about 50° C. and porosity of about 0.59%;
- at a temperature of 70° C. and porosity of about 0.48%;
- at a current density of about 300 mA/cm2 and porosity of about 0.53%;
- and at a current density is 200 mA/cm2 and porosity is about 0.41%.