Method for improvement of the consumption controlling performance of water-soluble electrolyte chemical cells and fuel cells
OwnerYasuo Sakakurainventor
Life of this patent
Estimating the term…
Abstract
The invention provides a hydrogen activating material, which includes as a major constituent an iron-semiconductor alloy containing iron and semiconductor components. It also provides a consumption controlling material for water-soluble electrolyte chemical cells and fuel cells. In addition a hydrogen activating method is also provided.
Claims4
A method of retaining a high voltage of water-soluble electrolyte chemical cells with regard to an iron-semiconductor alloy in the shape of a plate produced by addition of a semiconductor to molten iron during steel making and rolling under load, comprising locating the iron-semiconductor alloy in the vicinity of the water-soluble electrolyte chemical cells, then severely vibrating the semiconductor by irradiating the iron-semiconductor alloy, from which vibrating-electromagnetic waves are generated on the basis of electrochemical potentials across iron and semiconductor crystals, with sunlight or white light with wavelengths of from 1 nm to 1 mm, thereby enhancing vibrating-electromagnetic waves further generated from the alloy and retaining a high voltage of water-soluble electrolyte chemical cells in the vicinity of the alloy, wherein the content of the semiconductor is 1-10 weight percent and the content of iron is 78-98 weight percent.
A method of retaining a high voltage of fuel cells with regard to an iron-semiconductor alloy in the shape of a plate produced by addition of a semiconductor to molten iron during steel making and rolling under load, comprising locating the iron-semiconductor alloy in the vicinity of the fuel cells, then severely vibrating the semiconductor by irradiating the iron-semiconductor alloy, from which vibrating-electromagnetic waves are generated on the basis of electrochemical potentials across iron and semiconductor crystals, with sunlight or white light with wavelengths of from 1 nm to 1 mm, thereby enhancing vibrating-electromagnetic waves further generated from the alloy and retaining a high voltage of fuel cells in the vicinity of the alloy, wherein the content of the semiconductor is 1-10 weight percent and the content of iron is 78-98 weight percent.
Dependencies are inferred from the claim text.