White reflective coating for modified bitumen membrane
AssigneeBuilding Materials Investment Corporation
InventorsAmir Khan, Michael De Souto
Life of this patent
Estimating the term…
Abstract
A coating composition useful for building materials products, especially roofing surfaces, is provided. The coating composition provides durable exterior protection to surfaces that it applied to, and it has reflective properties. The coating composition includes a mixture of a polymeric binder, a polymeric carrier and a pigment. The pigment is present in the coating composition in amount that is capable of providing a coating that has an initial energy efficiency rating greater than or equal to 0.65 for a low-sloped roof, or an initial energy efficiency greater than or equal to 0.25 for a steep-sloped roof.
Claims14
A method of manufacturing a modified bitumen roofing membrane, the method comprising:
- providing an aqueous dispersion of a polymeric binder, a polymeric carrier and an effective amount of a pigment that is capable of providing a coating that has an initial energy efficacy rating greater than or equal to 0.65 for a low-sloped roof, or an initial energy efficacy greater than or equal to 0.25 for a steep-sloped roof;
- maintaining constant mixing of the aqueous dispersion under low shear conditions of about 60 rpm or less to create a top coating composition;
- applying said top coating composition in-plant to an exterior surface of a modified bitumen substrate during manufacture of the roofing membrane;
- and
- curing said top coating composition at the temperature of the environment in which the coated substrate is located.
A method of manufacturing a modified bitumen roofing membrane, the method comprising:
- (1) mixing the following ingredients as an aqueous dispersion under low shear conditions of about 60 rpm or less to create a top coating composition:
- (a) 2-40% water;
- (b) 0.1-0.6% potassium tripolyphosphate;
- (c) 0.1-7.0% sodium salt of a carboxylic acid;
- (d) 0.1-7.0% oil-based defoamer;
- (e) 5-60% binder;
- (f) 0.1-7% thickener;
- (g) 0.5-7.0% coalescing agent;
- (h) 5-45% alumina trihydrate;
- (i) 0.1-4% microbiocide;
- (j) 1-10% zinc borate;
- (k) 0.1-4% zinc oxide;
- (l) an effective amount of titanium dioxide that is capable of providing a coating that has an initial energy efficacy rating greater than or equal to 0.65 for a low-sloped roof, or an initial energy efficacy greater than or equal to 0.25 for a steep-sloped roof;
- and
- (2) applying said top coating composition in-plant to an exterior surface of a substrate during manufacture of the roofing membrane.
Dependencies are inferred from the claim text.