Process for producing scorodite and recycling the post-scorodite-synthesis solution
AssigneeJX Nippon Mining & Metals Corporation
InventorsYukio Kimura, Shigeo Katsura
Life of this patent
Estimating the term…
Abstract
The present invention is to provide a process for producing a scorodite that can shorten the time required for synthesizing the scorodite, and further can improve the yield of arsenic and iron into the scorodite. Accordingly, a process for producing a crystalline scorodite from an acidic aqueous solution containing pentavalent As and trivalent Fe, wherein the synthesis of the crystalline scorodite is performed after the molar ratio of trivalent Fe to pentavalent As contained in the acidic aqueous solution is adjusted to be equal to or more than 0.9 and equal to or less than 1.1 is provided.
Claims2
A process for recycling a post-scorodite-synthesis solution, comprising the steps of:
- (1) conducting a sulfuric acid leaching by feeding an oxygen-containing gas into an electrolytically precipitated copper in an acidic aqueous solution of sulfuric acid, while stirring the solution at a temperature and for a time sufficient for oxidizing As component contained in the electrolytically precipitated copper to pentavalent, followed by solid-liquid-separation of the solution into a post-leaching residue and a sulfuric acid-leached solution containing the pentavalent As component,
- (2) adding ferric sulfate into said sulfuric acid-leached solution so that the molar ratio of trivalent Fe to pentavalent As may be equal to or more than 0.9 and equal to or less than 1.1 to prepare a reaction solution, followed by synthesis of a crystalline scorodite,
- (3) after the synthesis of the scorodite, conducting solid-liquid-separation of the reaction solution into a post-scorodite-synthesis solution and a scorodite crystal, and
- (4) using the post-scorodite-synthesis solution directly as an electrolyte solution used in electrolytic refining of copper.
Dependencies are inferred from the claim text.