Method of providing paper-making fibers with durable curl and absorbent products incorporating same
AssigneeGeorgia-Pacific Consumer Products LP
InventorJeffrey A. Lee
Life of this patent
Estimating the term…
Loading patent…
AssigneeGeorgia-Pacific Consumer Products LP
InventorJeffrey A. Lee
Estimating the term…
A process for producing high bulk cellulosic fiber exhibiting a durable elevated curl index includes: (a) concurrently heat treating and convolving cellulosic fiber pulp at elevated temperature and pressure at high consistency under conditions selected so as to preclude substantial fibrillation and attendant paper strength and fiber bonding development; and (b) recovering the pulp wherein the length weighted curl index of the treated fiber is at least about 20% higher than the length weighted curl index of the fiber prior to the heat treatment and convolving thereof. The curl imparted to the fiber persists upon treatment for 30 minutes in a laboratory disintegrator at 3000 rpm at 1% consistency at a temperature of 125° F. Moreover, the curl may be imparted to the fiber in a disk refiner at very short residence times, on the order of several seconds or less. In general, the process is carried out in the presence of saturated steam at a pressure of from about 5 to about 150 psig.
An absorbent sheet comprising a heat-treated and convolved fiber having a length weighted curl index at least about 40% higher than the fiber prior to being heat-treated and convolved, the at least 40% elevation of the length weighted curl index of the treated fiber being capable of persisting for at least 30 minutes in a disintegrator at 1% consistency at a temperature of 125° F., and the treated fiber having substantially the same strength as the fiber prior to being heat-treated and convolved, the absorbent sheet made by way of:
An absorbent sheet comprising a heat-treated and convolved fiber having a length weighted curl index at least about 40% higher than the fiber nor to being heat-treated and convolved, the at least 40% elevation of the length weighted curl index of the treated fiber being capable of persisting for at least 30 minutes in a disintegrator at 1% consistency at a temperature of 125° F., and the treated fiber having substantially the same strength as the fiber prior to being heat-treated and convolved, the absorbent sheet made by a process comprising:
An absorbent sheet comprising a heat-treated and convolved fiber having a length weighted curl index at least about 40% higher than the fiber prior to being heat-treated and convolved, the at least 40% elevation of the length weighted curl index of the treated fiber being capable of persisting for at least 30 minutes in a disintegrator at 1% consistency at a temperature of 125° F., and the treated fiber having substantially the same strength as the fiber prior to being heat-treated and convolved, the absorbent sheet made by a process comprising:
An absorbent sheet comprising a heat treated mechanically curled fiber having a length weighted curl index at least about 40% higher than the fiber prior to being heat-treated and convolved, the at least 40% elevation of the length weighted curl index of the treated fiber being capable of persisting for at least 30 minutes in a disintegrator at 1% consistency at a temperature of 125° F. and the treated fiber having substantially the same strength as the fiber prior to being heat-treated and convolved, wherein the fiber is made by a process comprising:
An absorbent sheet comprising a heat-treated and convolved fiber having a length weighted curl index at least about 40% higher than the fiber prior to being heat-treated and convolved, the at least 40% elevation of the length weighted curl index of the treated fiber being capable of persisting for at least 30 minutes in a disintegrator at 0.4% consistency at a temperature of 125° F., and the treated fiber having substantially the same strength as the fiber prior to being heat-treated and convolved, the absorbent sheet made by way of:
An absorbent sheet comprising a heat-treated and convolved fiber having a length weighted curl index at least about 40% higher than the fiber prior to being heat-treated and convolved, the at least 40% elevation of the length weighted curl index of the treated fiber being capable of persisting for at least 30 minutes in a disintegrator at 1% consistency at a temperature of 125° F., and the treated fiber having substantially the same strength as the fiber prior to being heat-treated and convolved, the absorbent sheet made by way of:
An absorbent sheet comprising a heat-treated and convolved fiber having a length weighted curl index at least about 40% higher than the fiber prior to being heat-treated and convolved, said at least 40% elevation of the length weighted curl index of the treated fiber being capable of persisting for at least 30 minutes in a disintegrator at 1% consistency at a temperature of 125° F., and said treated fiber having substantially the same fibrillation and attendant strength as the fiber prior to said treatment, the absorbent sheet made by way of:
Dependencies are inferred from the claim text.