Acidic group-containing solid inks
AssigneeXerox Corporation
InventorPinyen Lin
Life of this patent
Estimating the term…
Abstract
A microfluidic device includes a first substrate, and a phase change ink deposited on a surface of the first substrate. The phase change ink includes an ink vehicle including a polymeric material having one or more acidic groups, and an optional colorant, wherein the phase change ink is solid at room temperature but is liquid at a jetting temperature of from about 60 to about 150° C., and an acidic group mass percentage, measured as a total mass of acid groups to an entire weight of the ink, is from about 1% to about 35%.
Claims20
A microfluidic device comprising:
- a first substrate, and
- a phase change ink deposited on a surface of the first substrate, the phase change ink comprising an ink vehicle comprising a polymeric material having one or more acidic groups, and an optional colorant,
- wherein the phase change ink is solid at room temperature but is liquid at a jetting temperature of from about 60 to about 150° C., and
- an acidic group mass percentage, measured as a total mass of acid groups to an entire weight of the ink, is from about 1% to about 35%.
A microarray comprising:
- a substrate, and
- an image printed on the substrate using a phase change ink comprising an ink vehicle comprising a polymeric material having one or more acidic groups, and an optional colorant,
- wherein the phase change ink is solid at room temperature but is liquid at a jetting temperature of from about 60 to about 150° C., and an acidic group mass percentage, measured as a total mass of acid groups to an entire weight of the ink, is from about 1% to about 35%.
A method for making a microarray, comprising:
- providing a substrate;
- ejecting droplets of a phase change ink from an ink jet printer onto the substrate, to form an image;
- and
- allowing the image to solidify,
- wherein the phase change ink comprises an ink vehicle comprising a polymeric material having one or more acidic groups, and an optional colorant,
- the phase change ink is solid at room temperature but is liquid at a jetting temperature of from about 60 to about 150° C., and
- an acidic group mass percentage, measured as a total mass of acid groups to an entire weight of the ink, is from about 1% to about 35%.
Dependencies are inferred from the claim text.