Abstract
Systems and methods for pelletizing hot asphaltenes are provided. Asphaltenic hydrocarbons can be dispersed to provide two or more asphaltenic particles. The asphaltenic hydrocarbons can be at a temperature of from about 175° C. to about 430° C. The asphaltenic particles can be contacted with a film of cooling medium. The film can have a thickness of from about 1 mm to about 500 mm. At least a portion of the asphaltenic particles can be solidified by transferring heat from the asphaltenic particles to the cooling medium to provide solid asphaltenic particles. The solid asphaltenic particles can be separated from at least a portion of the cooling medium.
Claims15
A method for pelletizing hot asphaltenes, comprising:
- dispersing an asphaltenic hydrocarbon comprising a temperature of from about 175° C. to about 430° C. to provide two or more asphaltenic particles;
- pre-cooling the asphaltenic particles, the pre-cooling comprising passing the asphaltenic particles through a mist of cooling medium prior to contacting the asphaltenic particles with the film of cooling medium;
- contacting the pre-cooled asphaltenic particles with a film of cooling medium, the film comprising a thickness of from about 1 mm to about 500 mm;
- solidifying at least a portion of the asphaltenic particles by transferring heat from the asphaltenic particles to the cooling medium to provide solid asphaltenic particles;
- and
- separating the solid asphaltenic particles from at least a portion of the cooling medium.
A method for pelletizing hot asphaltenes, comprising:
- dispersing an asphaltenic hydrocarbon comprising a temperature of from about 175° C. to about 430° C. to provide two or more asphaltenic particles;
- pre-cooling the asphaltenic particles, the pre-cooling comprising passing the asphaltenic particles through a mist of cooling medium prior to contacting the asphaltenic particles with the film of cooling medium;
- cooling at least a portion of the pre-cooled asphaltenic particles using a film of cooling medium to provide solid asphaltenic particles, the film of cooling medium comprising a thickness of from about 1 mm to about 500 mm, wherein the asphaltenic particles are cooled at a rate of about 1° C./sec to about 50° C./sec;
- separating the solid asphaltenic particles from at least a portion of the cooling medium to provide a recovered cooling medium;
- and
- recycling at least a portion of the recovered cooling medium to provide at least a portion of the film of cooling medium.
Dependencies are inferred from the claim text.