Micronized wood preservative formulations comprising copper and zinc
AssigneeOsmose, Inc.
InventorsJun Zhang, Wenjin Zhang
Life of this patent
Estimating the term…
Abstract
Use of micronized zinc compounds in wood preservation treatments containing micronized copper compounds significantly increases the efficacy of the treatment with respect to that of the copper compounds alone. Micronized copper compounds used at a retention in the range of from 0.005 to 1 pounds per cubic foot (pcf) expressed as CuO equivalent, and zinc compounds are used at a retention in the range of from 0.005 to 1 pcf expressed as ZnO equivalent, the increase in wood preservation efficacy over similar retentions of copper compounds alone can be seen in as little as 24 months.
Claims21
A composition comprising:
- a) a particulate copper or copper compound component;
- b) a particulate zinc or zinc compound component;
- wherein at least 85 wt % of the particles are in the range of from .001 to 25 microns;
- and
- c) a polymeric dispersant, wherein the weight ratio of elemental copper to elemental zinc is in the range of from 15:1 to 1:15.
A method of preserving wood comprising the steps of:
- a) applying to the wood a composition comprising:
- 1) a particulate copper or copper compound component;
- and
- 2) a particulate zinc or zinc compound component;
- wherein at least 85 wt % of the particles are in the range of from 0.001 to 25 microns;
- and
- b) impregnating the wood with said particles such that the particulate copper or copper compound component is present at a wood retention in the range of from 0.005 to 1 pounds per cubic foot (pcf) CuO equivalents, and the particulate zinc or zinc compounds are present at a wood retention in the range of from 0.005 to 1 pounds per cubic foot (pcf) ZnO equivalents.
Wood comprising:
- 1) a particulate copper or copper compound component;
- and
- 2) a particulate zinc or zinc compound component;
- wherein at least 85 wt % of the particles are in the range of from 0.001 to 25 microns, such that the particulate copper or copper compound component is present at a wood retention in the range of from 0.005 to 1 pounds per cubic foot (pcf) CuO equivalents, and the particulate zinc or zinc compounds are present at a wood retention in the range of from 0.005 to 1 pounds per cubic food (pcf) ZnO equivalents.
Dependencies are inferred from the claim text.