Ring traveler and method for producing it
AssigneeBracker AG
InventorJörg Kägi
Life of this patent
Estimating the term…
Abstract
The present invention relates to a ring traveler (10) for ring spinning or ring twisting machines, with a core (20) consisting of a ferrous material, a covering layer (24) being arranged on at least parts of the core. The covering layer (24) in this case contains fine-crystalline chromium nitride, vanadium carbide or titanium carbonitride. As a result of the covering layer, the ring traveler according to the invention has good abrasion resistance and corrosion resistance.
Claims18
A ring traveler (10) for ring spinning or ring twisting machines, with a core (20) comprising a ferrous material, a covering layer (24) being arranged on at least parts of the core, wherein the covering layer contains a needle-like fine crystalline structure of a material selected from the group consisting of chromium nitride, vanadium carbide and titanium carbonitride.
A ring traveler (10) for ring spinning or ring twisting machines, with a core (20) consisting of a ferrous material, a covering layer (24) being arranged on at least parts of the core, wherein the covering layer (24) has a needle-like fine-crystalline structure consisting essentially of chromium nitride and vanadium carbide.
A method for producing a ring traveler (10) with a core (20) comprising ferrous material, at least parts of the core being covered with a covering layer (24) containing TiCN, CrN or VC, in which method the core is heated to 700° C to 1200° C. in a reaction chamber, a precipitation gas is introduced into the reaction chamber, so that a covering layer (24) is applied to the surface of the core, and the coated ring traveler is cooled, wherein the ring traveler is cooled under protective gas for 2 to 4 hours.
A method of forming a ring traveler (10) comprising the steps of:
- (a) providing a core (20) comprising a ferrous material;
- (b) heating the core (20) in a reaction chamber to between about 700° C. and 900° C;
- (c) introducing into the reaction chamber a precipitation gas consisting of CH3CN and TiCl4
- (d) precipitating a coating of the precipitation gas onto a surface of the core (2);
- and
- (e) cooling the coated core (20) under a protective gas for about 2 to 4 hours.
A ring traveler for ring spinning or ring twisting machines, with a core comprising a ferrous material, at least parts of the core being covered with a covering layer containing TiCN, CrN or VC, the ring traveler being coated by the steps of:
- heating the core to 700° C. to 1200° C. in a reaction chamber;
- introducing a precipitation gas into the reaction chamber, so that a covering layer is applied to the surface of the core;
- and cooling the ring traveler under protective gas for 2 to 4 hours.