Emollient carrier gel
AssigneeReact-NTI, LLC
InventorBruce Anthony Tavares
Life of this patent
Estimating the term…
Abstract
A waxy solid having ultrafine particles homogeneously distributed in a mixture of vegetable oil and waxy solid, the oil being present in a major proportion by weight, forms a homogeneous colloidal solution which is then cooled and subjected to high shear to form ultrafine particles of the waxy solid, in situ, in a size range from about 0.1 μm to 10 μm. The resulting stiff gel retains its shape and high viscosity for at least 30 days when confined in a container in an air atmosphere at 40° C. at substantially sea level. The stability of the gel is visually evidenced by a lack of syneresis. The gel is destabilized at a temperature in the range from 52° C. (125° F.) to 100° C. (212° F.).
Claims10
An essentially anhydrous, hydrophobic, substantially pigment free, homogeneous and stable carrier gel, free of synthetic oils, consisting of a minor proportion by weight of a waxy solid and a major proportion by weight of a naturally occurring vegetable oil, the gel being present as a colloid in which the dispersed phase of waxy solid particles has combined with the continuous phase of vegetable oil to produce a semi-solid material substantially free of any solvent, the gel having physical properties including viscosity, stability, emolliency and occlusivity similar to that of petrolatum so as to be a substitute for petrolatum but having a destabilization point in the range from 520° C. (125° F.) to 100° C. (212° F.).
A method for preparing a carrier gel, comprising,
- heating a mixture consisting of a minor proportion by weight of a waxy solid and a major proportion by weight of a vegetable oil substantially free of any solvent, to a temperature above the melting point of the waxy solid but below a temperature at which either of the components is degraded to form a homogeneous colloidal solution;
- cooling the mixture to a temperature below about 38° C. (100° F.) to form a slurry having an initial viscosity in the range from about 2,000 cp to 50,000 cp at 25° C.;
- continuously mixing the slurry with sufficient energy to raise the temperature at least 5° C. to form a rheopectic mass and simultaneously cooling the mass to a temperature below 49° C. (120° F.);
- thereafter cooling the rheopectic mass to ambient temperature;
- and,
- recovering a cool and stable carrier gel having physical properties similar to that of petrolatum so as to be a substitute for petrolatum but having a destabilization point in the range from 52° C. (125° F.) to 100° C. (212° F.).
An emollient carrier gel produced by heating a mixture consisting of a minor proportion by weight of a waxy solid and a major proportion by weight of a naturally occurring vegetable oil substantially free of any solvent, to a temperature above the melting point of the waxy solid but below a temperature at which either of the components is degraded to form a homogeneous colloidal solution;
- cooling the mixture to a temperature below about 38° C. (100° F.) to form a slurry having an initial viscosity in the range from about 2,000 cp to 50,000 cp at 25° C.;
- continuously mixing the slurry with sufficient energy to raise the temperature at least 5° C. to form a rheopectic mass and simultaneously cooling the mass to a temperature below 49° C. (120° F.);
- thereafter cooling the rheopectic mass to ambient temperature;
- and, recovering a cool and stable carrier gel having physical properties similar to that of petrolatum so as to be a substitute for petrolatum but having a destabilization point in the range from 52° C. (125° F.) to 100° C. (212° F.).
Dependencies are inferred from the claim text.