Back to results
US 6,787,061 B1Granted
Copper polish slurry for reduced interlayer dielectric erosion and method of using same
AssigneeIntel Corporation
InventorAnne E. Miller
Life of this patent
Estimating the term…
Abstract
Slurries for use in the chemical mechanical polishing (CMP) of copper and copper diffusion barriers that reduce pattern sensitive erosion of an underlying dielectric layer include at least one surfactant. Inclusion of surfactants, such as cetyltrimethylammonium bromide in a slurry mixture can reduce pattern sensitive erosion of dielectric materials such as silicon oxide, and fluorinated oxides of silicon that would otherwise occur during CMP of copper and copper diffusion barriers as is typical in the formation of copper interconnect lines in integrated circuits.
Claims14
A copper polish slurry, comprising a mixture of:
- a surfactant comprising an alkyltrimethylammonium halide;
- a chelating buffer system;
- an abrasive comprising silica;
- an oxidizer;
- and a corrosion inhibitor;
- wherein the slurry has a pH between 2.5 and 7.0.
3 more elements
Dependencies are inferred from the claim text.