Highly ductile reduced imperfection weld for ductile iron and method for producing same
AssigneeU.S. Pipe and Foundry Company
InventorsDaniel A. Copeland, David J. Farr, James E. Wren
Life of this patent
Estimating the term…
Loading patent…
AssigneeU.S. Pipe and Foundry Company
InventorsDaniel A. Copeland, David J. Farr, James E. Wren
Estimating the term…
The art has experienced difficulty obtaining “sound” welds with high-nickel welds above the second pass. Particular problems are tension anomalies and sub-optimal interweld pass fusion at higher order passes of the weld wire, along with undesirably high heat levels transferred to the workpiece. The inventors have discovered that ductile iron-to-ductile iron welds can be reliably formed at mission-critical junctures by compensating for the brittle nature of the heat affected zone through enhancing ductility of the weld itself. The present invention provides in continuing part for a highly durable weld without soundness problems such as tension anomalies, multilayer fusion imperfections, or pinholes; and a method of forming such a weld. The weld is created using high nickel weld wire (filler metal or consumable electrode, or both) welded in a pure inert gas (or mixture of pure inert gasses and even reducing gasses). Additions of weld metal alloys, flux coring, and deoxidizing coatings are not required. The work pieces do not require pre- or post-heat treatment to minimize the effects of the HAZ. Additional inventive features are described more fully below.
A weld joint comprising a first workpiece, a second workpiece, and a weld body joining said first workpiece and said second workpiece, which weld body comprises lag-free weld puddle of substantially pure nickel that yields a weld joint substantially free of porosity.
A weld joint comprising a first workpiece, a second workpiece, and a weld body joining said first workpiece and said second workpiece, said weld body comprising an area attributable to a higher order pass that comprises substantially pure nickel, the surface of which is substantially free of slag and slag residuals, and which surface exhibits an average of four or fewer pits visible to a naked eye per square inch.
A weld comprising a higher order pass, and having a gradient of nickel purity as measured along a throat of said weld that generally increases between a root of said weld and a point within said higher order pass, said higher order pass being weldable with another weld pass without removal of slag.
A weld comprising a second order pass and a plurality of higher order passes, said plurality of higher order passes comprising at least a third order pass and a fourth order pass, the weld having a gradient of nickel purity that generally increases from a second order pass through said third order pass and said fourth order pass, and being substantially free of porosity and of slag.
A weld comprising a higher order pass, and having a gradient of nickel purity as measured along a throat of said weld that generally increases as the distance from a root of said weld increases, a face of said weld having an average of four or fewer pits visible to a naked eye per square inch, said face being substantially free of slag.
A slag-free weld comprising a plurality of passes, which passes comprise a second order pass and at least one higher order pass;
A method of producing a highly ductile weld, comprising the steps of:
A method of producing a highly ductile weld, comprising the steps of:
A method of creating a welded ductile iron joint having a yield strength of less than a tensile strength of a heat affected zone in said ductile iron joint, comprising compensating for a brittleness of said heat affected zone by creating a highly ductile weld bead in the absence of flux using a filler metal or a consumable electrode of a high ductility material consisting essentially of nickel.
Dependencies are inferred from the claim text.