Extruded multiphase bars exhibiting artisan-crafted appearance
AssigneeUnilever Home & Personal Care USA, Division of Conopco, Inc.
InventorsMichael Paul Aronson, Badreddine Ahtchi-Ali, Sergio Roberto Leopoldino, Gregory Jay Mc Fann, Mariangela Gomes de Oliveira Sichmann
Life of this patent
Estimating the term…
Abstract
The present invention relates to a process for making a multiphase personal wash bar having artisan crafted appearance. The bars are made by combining the second solid mass phase to a first continuous phase wherein the hardness of the second phase is at least twice the hardness of noodles forming the continuous phase.
Claims20
A multi phase extruded soap bar having an artisan-crafted appearance comprising:
- a) a continuous solid phase comprising 25-85% of a surfactant base suitable for cleansing the skin,
- b) domains of a discontinuous phase that comprises a water soluble or water dispersible solid matrix comprising at least 1 wt % surfactant wherein said discontinuous phase has its longest dimension between 3 and about 70 mm,
- wherein the hardness of the continuous phase is in the range of 1.9 to 2.5 bar when measured at a temperature between 33 and 50° C.;
- the ratio, λ, defines altered rheological phases wherein the hardness of the discontinuous phase measured at a temperature of 25° C. divided by the hardness of the continuous phase measured at a temperature of 33° C. is greater than 2.0 and wherein said hardness values are measured by the Cylinder Impaction Test,
- wherein the discontinuous phase comprises 1 to about 25 wt % of the bar, and
- wherein the bar has a descriptive visual grading score of at least 3.0 when measured by Visual Discrimination Panel Test;
- wherein the temperatures noted approximately reflect the thermal conditions of each phase when the continuous and discontinuous phases are first combined prior to final extrusion to form the composite mass.
A multiphase extruded soap bar having an artisan-crafted appearance comprising
- a) a continuous phase comprising:
- i) 25 to 85% of a surfactants base consisting of fatty acid soaps, syndets, and their mixtures,
- ii) 0.1 to 15% of a plasticizing agent selected from the group consisting of ester oils, hydrocarbon oils, silicone oil, fatty acids, fatty alcohol, waxes, nonionic surfactants, triethanolamine, glycerol, propylene glycol, and mixtures thereof
- b) a discontinuous solid phase having its longest dimension between 3 and about 45 mm comprised of,
- i) at least 1 wt % of a surfactant,
- ii) 5-95 wt % of a water soluble or water dispersible solid matrix selected from the group consisting fatty acid soap, polyethylene glycol having a melting point greater than 35° C., fatty acid, fatty alcohol, fatty esters, starch, maltodextran, and mixtures thereof,
- iii) 0.25-15 wt % of a hardening agent selected from the group consisting of polyols, polyethers, monovalent chlorides, monovalent and divalent sulfates, sodium carbonate, monovalent aluminates, monovalent phosphates, monovalent polyphosphates, silica, alumina, talc, and mixture thereof
- wherein the hardness of the continuous phase is in the range of 1.9 to 2.5 bar when measured at a temperature between 33 and 42° C., the ratio, λ, defines altered rheological phases wherein the hardness of the discontinuous phase measured at a temperature of 25° C. divided by the hardness of the continuous phase measured at a temperature of 33° C. is greater than 2.0 and wherein said hardness values are measured by the Cylinder Impaction Test,
- wherein the discontinuous phase comprises 1 to about 25 wt % of the bar, and
- wherein the bar has a descriptive visual grading score of at least 3.0 when measured by Visual Discrimination Panel Test;
- wherein the temperatures noted approximately reflect the thermal condition of each phase when the continuous and discontinuous phases are first combined prior to final extrusion to form the composite mass.
Dependencies are inferred from the claim text.