Cofireable dielectric composition
AssigneeMotorola, Inc.
InventorXunhu Dai
Life of this patent
Estimating the term…
Loading patent…
AssigneeMotorola, Inc.
InventorXunhu Dai
Estimating the term…
An exemplary composition of matter and method for making high-efficiency, low-loss capacitors is disclosed as including inter alia a B2O3—Bi2O3—ZnO glass in admixture with material typically comprising about 30-40 wt % cubic phase (Bi0.5Zn0.5)(Zn0.5Nb1.5)O7 and about 60-70 wt % pseudo-orthorhombic phase Bi2(Zn1/3Nb1/3)2O7 (e.g., “BZN”). The mixture effectively reduces the sintering temperature of BZN from the range of about 950-1050° C. to the range of about 850-900° C., thereby rendering BZN suitable for cofiring with, for example, existing LTCC dielectrics. Disclosed features and specifications may be variously controlled, configured, adapted or otherwise optionally modified to further improve or otherwise optimize the sintering temperature of BZN and/or BZN-based materials. Exemplary embodiments of the present invention representatively provide for embedded high-efficiency, low-loss capacitors that may be readily integrated with existing portable ceramic technologies for the improvement of dielectric properties, device package form factors, weights and/or other manufacturing, device or material performance metrics.
A method for reducing the sintering temperature of BZN without substantial degradation of the dielectric properties of the same, the method comprising the steps of:
A method for forming a high efficiency, low loss embedded capacitor, the method comprising the steps of:
A composition of matter for reducing the sintering temperature of BZN, said composition comprising a B2O3—Bi2O3—ZnO glass in admixture with BZN.
Dependencies are inferred from the claim text.