Cesium halide storage phosphor with narrow emission spectrum upon UV-excitation
AssigneeAfga-Gevaert Aktiengesellschaft
InventorsPaul Leblans, Luc Struye
Life of this patent
Estimating the term…
Abstract
A CsBr:Eu phosphor showing a narrow emission spectrum upon UV-excitation and panels including such a phosphor are disclosed. Also methods for preparing such a phosphor have been described.
Claims8
A CsBr:Eu phosphor showing upon excitation with light of 370 nm at a wavelength of λmax a maximum emission intensity I0 and at λmax +30 nm an emission intensity I, such that I≦0.20 I0.
A method for preparing a CsBr:Eu phosphor comprising the steps of:
- mixing or combining CsBr with between 10−3 mol % and 5 mol % of a europium compound wherein said europium compound is a member selected from the group consisting of EuX′2 EuX′3 and EuOX′, X′ being selected from the group consisting of F, Cl, Br, I and combinations thereof,
- heating said mixture at a temperature above 450° C.;
- cooling said mixture to room temperature,
- bringing said mixture after cooling to a temperature between 80 and 220° C. and
- maintaining said mixture at that temperature for a time between 10 minutes and 15 hours.
A method for preparing a CsBr:Eu phosphor comprising the steps of:
- mixing or combining CsBr with between 10−3 mol % and 5 mol % of a europium compound wherein said europium compound is a member selected from the group consisting of EuX′2 EuX′3 and EuOX′, X′ being selected from the group consisting of F, Cl, Br, I and combinations thereof,
- heating said mixture at a temperature above 450° C.;
- cooling said mixture to a temperature between 80 and 220° C. maintaining said mixture at that temperature for between 10 minutes and 15 hours;
- and
- cooling said mixture to room temperature.
A method for producing a binderless CsBr:Eu phosphor screen comprising the steps of:
- mixing or combining CsBr with between 10−3 mol % and 5 mol % of a europium compound wherein said europium compound is a member selected from the group consisting of EuX′2 EuX′3 and EuOX′, X′being selected from the group consisting of F, Cl, Br, I and combinations thereof,
- vapour depositing that mixture onto a substrate, forming a binderless phosphor screen,
- cooling said phosphor screen to room temperature,
- bringing said phosphor screen to a temperature between 80 and 220° C. and
- maintaining it at that temperature for between 10 minutes and 15 hours.
A method for preparing a binderless CsBr:Eu phosphor screen comprising the steps of:
- mixing or combining CsBr with between 10−3 mol% and 5 mol% of a europium compound wherein said europium compound is a member selected from the group selected from EuX′2, EuX′3 and EuOX′, X′ being selected from the group consisting of F, Cl, Br, I and combinations thereof,
- vapor depositing that mixture onto a substrate, forming a binderless phosphor screen;
- cooling said screen to a temperature between 80 and 220° C.;
- maintaining it at that temperature for between 10 minutes and 15 hours;
- and
- cooling said screen to room temperature.