Abstract
A fire retardant building material composed of a mixture of water and cellulose fibers, both of which can be comprised of readily available materials at the job site, such as the available water supply or natural water and scrap shredded paper, including newspaper or other discarded paper or cardboard materials. The water and cellulose fiber is mixed to form a slurry and calcium hydroxide, alumina, salt and ammonia are added. Pigments and aggregates may be added for appearance.
Claims17
A method of making a construction material comprising:
- a. Mixing water and cellulose fibers to form a slurry;
- b. Mixing salt into the slurry;
- c. Mixing ammonia into the slurry;
- d. Mixing calcium hydroxide into the slurry;
- and
- e. Mixing alumina into the slurry,
- wherein the ratio of calcium hydroxide to salt is approximately 25 to 1, by weight, and the ratio of calcium hydroxide to ammonia is approximately 25 to 1, by weight.
4 more elements
A method of making a construction material comprising:
- a. Mixing water and cellulose fibers to form a slurry;
- b. Mixing salt into the slurry;
- c. Mixing ammonia into the slurry;
- d. Mixing calcium hydroxide into the slurry;
- and
- e. Mixing alumina into the slurry,
- wherein the various components comprise approximately the following formula:
- 6 kilogram of cellulose fibers;
- 1 liter of ammonia (NH4);
- 1 liter of alumina;
- 1 liter of salt (NaCl);
- 25 kilograms of calcium hydroxide (CaOH);
- and
- 180 liters of water.