Abstract
The invention is a polymer resin that includes between about 20 and 200 ppm of an inert particulate additive, preferably selected from the group consisting of surface-modified talc and surface-modified calcium carbonate. The polymer resin is capable of being formed into low-haze, high-clarity bottles and films possessing reduced coefficient of friction.
Claims28
A polymer resin having reduced frictional properties, the polymer resin comprising between about 20 and 150 ppm of an inert particulate additive selected from the group consisting of talc and calcium carbonate, the inert particulate additive having an average particle size of less than about ten microns;
- wherein the polymer resin is selected from the group consisting of high-density polyethylene, low-density polyethylene, linear low-density polyethylene, polypropylene, polyvinyl chloride, and polyvinyl dichloride.
A polymer resin having reduced frictional properties, the polymer resin comprising between about 20 and 150 ppm of an inert particulate additive selected from the group consisting of surface-modified talc and surface-modified calcium carbonate, the inert particulate additive having an average particle size of less than about two microns;
- wherein the polymer resin is selected from the group consisting of high-density polyethylene, low-density polyethylene, linear low-density polyethylene, polyvinyl chloride, and polyvinyl dichloride.
A polymer resin having reduced frictional properties, the polymer resin comprising a polymer selected from the group consisting of high-density polyethylene, low-density polyethylene, linear low-density polyethylene, polyvinyl chloride, and polyvinyl dichloride, the polymer resin characterized by the inclusion of between about 40 and 100 ppm of an inert particulate additive selected from the group consisting of surface-modified talc end surface-modified calcium carbonate, the inert particulate additive having an average particle size of lens than about two microns.
Dependencies are inferred from the claim text.