High dielectric constant very low fired X7R ceramic capacitor, and powder for making
AssigneeMRA Laboratories, Inc.
InventorsGaleb H. Maher, Samir Maher
Life of this patent
Estimating the term…
Loading patent…
AssigneeMRA Laboratories, Inc.
InventorsGaleb H. Maher, Samir Maher
Estimating the term…
A dielectric ceramic powder and multilayer ceramic capacitors made from the powders are disclosed. A dielectric start powder mixture includes at least ninety weight percent essentially pure barium titanate powder having an average particle size of from 0.2 to 1.2 microns; from 0.2 to 2.5 weight percent of barium lithium borosilicate; from 0.1 to 0.3 weight percent of MnCO3; 0.4 to 1.50 weight percent Nb205 or a niobate compound, or a molar equivalent of Ta2O5 or a tantalum compound as a grain growth inhibitor; and, 0.4 to 1.2 weight percent of gadolinium oxide (Gd2O3). The start powder mixture is calcined and then sintered in an open zirconia setter at from 950° C. to 1,025° C. to produce a dielectric ceramic body that satisfies X7R capacitor performance characteristics; that includes no hazardous heavy metal oxides; and, that may include silver-palladium electrodes having 85 weight percent or more of silver.
A dielectric ceramic start powder comprising:
A method for making a dielectric ceramic powder comprising the steps of:
A method for making a multilayer ceramic capacitor that satisfies X7R capacitor performance characteristics, comprising the steps of:
A multilayer ceramic capacitor that satisfies X7R capacitor performance characteristics having a least one electrode buried within a body of the capacitor, and an external terminal connected to the at least one electrode, the body comprising:
Dependencies are inferred from the claim text.