Method of extending the stability of a photoresist during direct writing of an image upon the photoresist
AssigneeApplied Materials, Inc.
InventorsMelvin Warren Montgomery, Cecilia Annette Montgomery
Life of this patent
Estimating the term…
Loading patent…
AssigneeApplied Materials, Inc.
InventorsMelvin Warren Montgomery, Cecilia Annette Montgomery
Estimating the term…
In photomask making, the environmental sensitivity of a chemically amplified photoresist is eliminated, or at least substantially reduced, by overcoating the photoresist with a thin coating (topcoat) of a protective but transmissive material. To provide improved stability during the long time period required for direct writing of a photomask pattern, typically in the range of about 20 hours, the protective topcoat material is pH adjusted to be as neutral in pH as possible, depending on other process variable requirements. For example, a pH adjusted to be in the range from about 5 to about 8 is particularly helpful. Not only is the stability of the chemically amplified photoresist better during direct writing when the protective topcoat is pH adjusted, but a photoresist-coated substrate with pH adjusted topcoat over its surface can be stored longer prior to imaging without adverse consequences.
In a method of photomask making, a method of providing stability of a chemically amplified photoresist during the direct writing of a patterned image into said photoresist, comprising:
A method for preparing a photomask, comprising:
A method of maintaining feature critical dimension and uniformity during the fabrication of a photomask, comprising:
Dependencies are inferred from the claim text.