Thermal insulating and acoustic absorption coating
AssigneeVan Etten Holdings, Inc.
InventorMatthew Niemiec
Life of this patent
Estimating the term…
Abstract
A multifunctional thermochemically cured coating which provides noise reduction and weight reduction in combination with thermal insulating and corrosion resistant properties. The composition comprises an epoxy resin with a weight per epoxide of 175 to 950, a mixed methyl-phenyl hydroxyl functional silicone polymer, a catalyst, a silane, an anti-corrosive pigment, an inert film reinforcing pigment, calcium silicate fibers, a mixture of ground synthetic silicone rubber, silica, and fillers, and an organic solvent.
Claims49
A cured, thermal insulating, corrosion resisting and noise reducing coating composition comprising:
- a. an epoxy resin with a weight per epoxide of 175 to 950 ranging from about 9-12% of the total weight of the composition;
- b. a mixed methyl-phenyl functional silicone polymer ranging from about 13-17% of the total weight of the composition;
- c. a catalyst ranging from about 1-7% of the total weight of the composition;
- d. a silane ranging from about 1-3% of the total weight of the composition;
- e. an anti-corrosive pigment ranging from about 5-15% of the total weight of the composition;
- f. an inert film reinforcing pigment ranging from about 6-10% of the total weight of the composition;
- g. a plurality of calcium silicate fibers ranging from about 4-8% of the total weight of the composition;
- h. a mixture of synthetic silicone rubber, silica and fillers ranging from about 10-20% of the total weight of the composition;
- and
- i. an organic solvent ranging from about 5-50% of the total weight of the composition.
A thermochemically cured, thermal insulating, corrosion resisting and noise reducing coating composition comprising:
- a. an epoxy resin with a weight per epoxide of 175 to 950 ranging from about 9-11% of the total weight of the composition;
- b. a mixed methy-phenyl functional silicone polymer ranging from about 13-17% of the total weight of the composition.
- c. an organometallic catalyst ranging from about 1-7% of the total weight of the composition;
- d. a silane ranging from about 1-3% of the total weight of the composition;
- e. an anti-corrosive pigment ranging from about 5-15% of the total weight of the composition;
- f. an inert film reinforcing pigment ranging from about 6-10% of the total weight of the composition;
- g. a plurality of calcium silicate fibers ranging from about 4-8% of the total weight of the composition;
- h. a mixture of synthetic silicone rubber, silica and fillers ranging from about 10-20% of the total weight of the composition;
- i. an organic solvent ranging from about 5-50% of the total weight of the composition;
- j. a color changing pigment ranging from about 5-15% of the total weight of the composition;
- k. a thickening agent ranging from about ½-1% of the total weight of the composition;
- l. a anti-settling agent ranging from about ½-1% of the total weight of the composition;
- and
- m. a wetting agent ranging from about ½-3% of the total weight of the composition.
A method of applying a thermal insulating, corrosion resisting and noise reducing coating composition to a substrate comprising the steps of:
- (a) cleaning the substrate surface;
- (b) choosing a coating composition comprising an epoxy resin with a weight per epoxide of 185 to 950 ranging from about 9-11% of the total weight of the composition;
- a mixed methyl-phenyl functional silicone polymer ranging from about 13-17% of the total weight of the composition;
- an organometallic catalyst ranging from about 1-7% of the total weight of the composition;
- a silane ranging from about 1-3% of the total weight of the composition;
- an anti-corrosive pigment ranging from about 5-15% of the total weight of the composition;
- an inert film reinforcing pigment ranging from about 6-10% of the total weight of the composition;
- a plurality of calcium silicate fibers ranging from about 4-8% of the total weight of the composition;
- a mixture of synthetic silicone rubber, silica and fillers ranging from about 10-20% of the total weight of the composition;
- an organic solvent ranging from about 5-50% of the total weight of the composition;
- a color changing pigment ranging from about 5-15% of the total weight of the composition;
- a thickening agent ranging from about ½-1% of the total weight of the composition;
- a anti-settling agent ranging from about ½-1% of the total weight of the composition;
- and a wetting agent ranging from about ½-3% of the total weight of the composition;
- (c) applying the coating to the substrate surface by a spray process;
- and
- (d) heating the substrate to at least 400 degrees Fahrenheit for at least twenty (20) minutes.
A method of applying a thermal insulating, corrosion resisting and noise reducing coating composition to a substrate surface comprising the steps of:
- a. cleaning the substrate surface;
- b. choosing a coating composition comprising an epoxy resin with a weight per epoxide of 185 to 950 ranging from about 9-11% of the total weight of the composition;
- a mixed methyl-phenyl functional silicone polymer ranging from about 13-17% of the total weight of the composition;
- an catalyst that is reactant with an expoxide group, said catalyst ranging from about 1-7% of the total weight of the composition;
- a silane ranging from about 1-3% of the total weight of the composition;
- an anti-corrosive pigment ranging from about 5-15% of the total weight of the composition;
- an inert film reinforcing pigment ranging from about 6-10% of the total weight of the composition;
- a plurality of calcium silicate fibers ranging from about 4-8% of the total weight of the composition;
- a mixture of synthetic silicone rubber, silica and fillers ranging from about 10-20% of the total weight of the composition;
- an organic solvent ranging from about 5-50% of the total weight of the composition;
- a color changing pigment ranging from about 5-15% of the total weight of the composition;
- a thickening agent ranging from about ½-1% of the total weight of the composition;
- a anti-settling agent ranging from about ½-1% of the total weight of the composition;
- and a wetting agent ranging from about ½-3% of the total weight of the composition;
- c. applying the coating composition to the substrate surface by a spray process;
- and
- d. allowing the substrate to cure at room temperature for at least sixty (60) minutes.
Dependencies are inferred from the claim text.