α+β type titanium alloy, process for producing titanium alloy, process for coil rolling, and process for producing cold-rolled coil of titanium alloy
OwnerHideto Oyama, Takayuki Kida +2inventors
InventorsHideto Oyama, Takayuki Kida, Kazumi Furutani, Masamitsu Fujii
Life of this patent
Estimating the term…
Abstract
A high strength and ductility α+β type titanium alloy, comprising at least one is isomorphous β stabilizing element in a Mo equivalence of 2.0-4.5 mass %, at least one eutectic β stabilizing element in an Fe equivalence of 0.3-2.0 mass %, Si in an amount of 0.1-1.5 mass %, and C in an amount of 0.01-0.15% mass, and has a β transformation temperature no lower than 940° C.
Claims18
An α+β titanium alloy comprising at least one isomorphous β-stabilizing element in a Mo equivalence of 2.0-4.5 mass %, at least one eutectic n-stabilizing element in an Fe equivalence of 0.3-2.0 mass %, Si in an amount of 0.1-1.5 mass %, and C in an amount of 0.01-0.15 mass %, and has a β transformation temperature no lower than 940° C.
An α+β titanium alloy comprising at least one isomorphous β-stabilizing element in a Mo equivalence of 2.0-4.5 mass %. at least one eutectic β-stabilizing element in an Fe equivalence of 0.3-2.0 mass %. Si in an amount of 0.1-1.5 mass %. and C in an amount of 0.01-0.15 mass %. wherein the alloy contains O as an additional element such that the amount of Mo-equivalence, the amount of Fe-equivalence, and the content of O satisfy the following inequality [1]:
- 7.0 mass %≦(Mo-equivalence+2.5×Fe-equivalence+40×O mass %)≦19 mass % [1].
An α+β titanium alloy comprising at least one isomorphous β-stabilizing element in a Mo equivalence of 2.0-4.5 mass %. at least one eutectic β-stabilizing element in an Fe equivalence of 0.3-2.0 mass %, Si in an amount of 0.1-1.5 mass %, and C in an amount of 0.01-0.15 mass %, wherein the alloy further contains a platinum group element in an amount of 0.03-0.2 mass %.
A process for rolling an α+β titanium alloy comprising at least one isomorphous β-stabilizing element in a Mo equivalence of 2.0-4.5 mass %. at least one eutectic β-stabilizing element in an Fe equivalence of 0.3-2.0 mass %, Si in an amount of 0.1-1.5 mass %, and C in an amount of 0.01-0.15 mass %, said process comprising:
- annealing the titanium alloy at a temperature (T2) which satisfies the following inequality [3]
- [β-transus−270° C.]≦T2≦(β-transus−50° C.) [3]:
- and then rolling the annealed titanium alloy.
A process for annealing a cold-rolled coil of an α+β titanium alloy comprising at least one isomorphous β-stabilizing element in a Mo equivalence of 2.0-4.5 mass %, at least one eutectic β-stabilizing element in an Fe equivalence of 0.3-2.0 mass %, Si in an amount of 0.1-1.5 mass %, and C in an amount of 0.01-0.15 mass %, characterized in that the heating temperature for annealing is higher than the temperature at which work hardening due to cold-rolling is relieved and lower than the β transus but excludes the temperature range in which a alloy of brittle hexagonal crystals emerges, thereby improving the elongation in the transverse direction of the rolled strip of the titanium alloy.
Dependencies are inferred from the claim text.