Methods to partially reduce a niobium metal oxide and oxygen reduced niobium oxides
AssigneeCabot Corporation
InventorJames A. Fife
Life of this patent
Estimating the term…
Abstract
Methods to at least partially reduce a niobium oxide are described wherein the process includes heat treating the niobium oxide in the presence of a getter material and in an atmosphere which permits the transfer of oxygen atoms from the niobium oxide to the getter material, and for a sufficient time and at a sufficient temperature to form an oxygen reduced niobium oxide. Niobium oxides and/or suboxides are also described as well as capacitors containing anodes made from the niobium oxides and suboxides.
Claims42
A method to at least partially reduce a niobium oxide comprising heat treating the niobium oxide in the presence of a getter material and in an atmosphere which permits the transfer of oxygen atoms from the niobium oxide to the getter material, for a sufficient time and temperature to form an oxygen reduced niobium oxide, wherein said getter material comprises tantalum, niobium, tantalum hydride particles, or combinations thereof, wherein said atmosphere comprises a hydrogen atmosphere.
A niobium oxide having an atomic ratio of niobium to oxygen of 1:less than 1.5, wherein said niobium oxide has a specific surface area of from 0.5 to about 10.0 m2/g.
A niobium oxide comprising an atomic ratio of niobium to oxygen of 1:less than 2.5, and further comprising nitrogen, wherein said niobium oxide has a specific surface area of from about 0.5 to about 10.0 m2/g and/or an apparent density of less than about 2.0 g/cc.