A method for changing the dielectric properties of a polymer impregnated and pyrolyzed ceramic matrix composite (polymer impregnated and pyrolyzed ceramic matrix composite) is disclosed. The polymer impregnated and pyrolyzed ceramic matrix composite can be used in aircraft and turbine engines. polymer impregnated and pyrolyzed ceramic matrix composite comprises a ceramic matrix, a reinforcing fiber, and at least 1 additive used to change dielectric properties (dielectric constant and loss factor). The additive can be a low dielectric constant material having a dielectric constant in the range of 1 to 7.5. The low dielectric constant material can be an oxide such as silica or aluminosilicate or a non-oxide such as silicon nitride, boron nitride, or silicon carbide. The low dielectric constant material can be incorporated in the ceramic matrix as a filler. The low dielectric constant material may be incorporated in a uniform array of holes fabricated in the polymer impregnated and pyrolyzed ceramic matrix composite.
A method for changing dielectric properties of a polymer impregnated and pyrolyzed matrix composite, wherein the method comprises
A method for fabricating a polymer impregnated and pyrolyzed ceramic matrix composite, wherein the method comprises:
A method for changing the dielectric properties of a polymer impregnated and pyrolyzed ceramic matrix composite, wherein the method comprises fabricating a uniform array of holes having a diameter in the range of 0.0254 to 0.254 cm in the polymer impregnated and pyrolyzed ceramic composite, which comprises a reinforcing fiber, ceramic matrix and filler.