Technique for reducing the cold flow of rubbers
AssigneeThe Goodyear Tire & Rubber Company
InventorsWen-Liang Hsu, Adel Farhan Halasa
Life of this patent
Estimating the term…
Loading patent…
AssigneeThe Goodyear Tire & Rubber Company
InventorsWen-Liang Hsu, Adel Farhan Halasa
Estimating the term…
Cold flow is a problem that is commonly encountered in the handling and storage of low molecular weight linear rubbers, such as low vinyl polybutadiene rubber and isoprene-butadiene rubber. This invention is based upon the unexpected discovery that the cold flow of such rubbery polymers can be greatly reduced by incorporating a small block of polystyrene therein. The rubbery polymers of this invention which exhibit a low level of cold flow can be synthesized by simply terpolymerizing 1,3-butadiene, isoprene and from about 0.5 phm to about 3 phm of styrene under anionic polymerization conditions in the absence of a polar modifier. It is preferred to utilize batch .polymerization techniques. However, continuous polymerization techniques can also be utilized. This invention more specifically disclosed a rubbery polymer which is comprised of polymer chains containing repeat units which are derived from 1,3-butadiene, isoprene and from about 0.5 weight percent to about 3 weight percent styrene, wherein the repeat units which are derived from styrene are in blocks at the ends of the polymer chains, wherein the rubbery polymer has a glass transition temperature which is within the range of about −105° C. to about −65° C. and wherein the rubbery polymer has a number average molecular weight which is within the range of about 50,000 to about 600,000.
A pneumatic tire having an outer circumferential tread wherein said tread is a sulfur-cured rubber composition comprised of, based on 100 parts by weight of rubber, (a) from about 30 to about 80 parts of a modified isoprene-butadiene rubber, wherein said modified isoprene-butadiene rubber is comprised of polymer chains containing repeat units which are derived from 1,3-butadiene, isoprene and from about 0.5 weight percent to about 3 weight percent styrene, wherein the repeat units which are derived from styrene are in blocks at the ends of the polymer chains, wherein the modified isoprene-butadiene rubber has a glass transition temperature which is within the range of about −105° C. to about −65° C. and wherein the rubbery polymer has a number average molecular weight which is within the range of about 50,000 to about 600,000;
Dependencies are inferred from the claim text.