Electroslag surfacing using wire electrodes
AssigneeStoody Company
InventorsDaya Singh, Ravi Menon
Life of this patent
Estimating the term…
Abstract
A method for depositing corrosion and wear resistant high alloy overlayers on industrial component substrates. Dilution of alloying components from out of the overlayer into the substrate is minimized by use of electroslag surfacing onto horizontally positioned surfaces of the substrate using oscillating wire.
Claims15
A method for depositing a high alloy stainless steel overlayer onto a substrate comprising:
- oscillating between one and six wire electrodes above said substrate;
- feeding flux onto said substrate while applying a total current to said electrodes sufficient to create a molten slag pool and maintain said molten slag pool by ohmic heating of said flux to deposit said overlayer by electroslag surfacing onto said substrate;
- and
- mechanically restraining said flux and molten slag pool on said substrate with a leading edge barrier positioned such that fresh substrate onto which overlayer is to be deposited is rotated under said barrier prior to passing under said electrode.
A method for depositing a high alloy stainless steel overlayer onto an elongate cylindrical substrate comprising:
- securing the substrate horizontally in a fixture adapted to rotate the substrate about a horizontal axis thereof, the substrate having a circumference comprising a bottom arcuate segment, two side arcuate segments, and a top arcuate segment directly opposite and above the bottom arcuate segment;
- maintaining an electrode comprising at least one wire above said top arcuate segment of said substrate while feeding flux onto said top arcuate segment;
- applying a total current to said electrode sufficient to create a molten metal pool and a molten slag pool and maintain said molten slag pool by ohmic heating of said flux to deposit said overlayer onto the top arcuate segment of said substrate;
- and
- rotating said substrate about said horizontal axis to continually present fresh substrate to said electrode;
- wherein said electrode contains Ni and Cr and said overlayer comprises at least a first layer in contact with the substrate, wherein dilution of Ni and Cr in said first layer is less than about 25%.
A method for depositing a high alloy stainless steel overlayer onto a substrate comprising:
- maintaining between one and six wire electrodes above said substrate;
- and
- feeding flux onto said substrate while applying a total current to said electrodes sufficient to maintain a molten slag pool by ohmic heating of said flux to deposit said overlayer by electroslag surfacing onto said substrate;
- wherein said electrode contains Ni and Cr and said overlayer comprises at least a first layer in contact with the substrate, wherein dilution of Ni and Cr in said first layer is less than about 25%.
A method for depositing a high alloy stainless steel overlayer onto an elongate cylindrical substrate comprising:
- securing the substrate horizontally in a fixture adapted to rotate the substrate about a horizontal axis thereof, the substrate having a circumference comprising a bottom arcuate segment, two side arcuate segments, and a top arcuate segment directly opposite and above the bottom arcuate segment;
- maintaining an electrode comprising at least one wire above said top arcuate segment of said substrate while feeding flux onto said top arcuate segment;
- applying a total current to said electrode sufficient to maintain a molten slag pool by ohmic heating of said flux to deposit said overlayer onto the top arcuate segment of said substrate;
- rotating said substrate about said horizontal axis to continually present fresh substrate to said electrode;
- and
- mechanically restraining said flux and molten slag pool on said substrate with a leading edge barrier positioned such that fresh substrate onto which overlayer is to be deposited is rotated under said barrier prior to passing under said electrode.
A method for depositing a high alloy stainless steel overlayer onto an elongate cylindrical substrate comprising:
- securing the substrate horizontally in a fixture adapted to rotate the substrate about a horizontal axis thereof, the substrate having a circumference comprising a bottom arcuate segment, two side arcuate segments, and a top arcuate segment directly opposite and above the bottom arcuate segment;
- maintaining an electrode comprising at least one wire above said top arcuate segment of said substrate while feeding flux onto said top arcuate segment;
- applying a total current to said electrode sufficient to maintain a molten slag pool by ohmic heating of said flux to deposit said overlayer onto the top arcuate segment of said substrate;
- rotating said substrate about said horizontal axis to continually present fresh substrate to said electrode;
- and
- applying a vacuum pick up above said slag pool to remove unmelted flux therefrom and to increase air flow around said slag pool to speed cooling thereof and thereby reduce the tendency of said slag pool to roll off said top arcuate segment;
- wherein said electrode contains Ni and Cr and said overlayer comprises at least a first layer in contact with the substrate, wherein dilution of Ni and Cr in said first layer is less than about 25%.
A method for depositing a high alloy stainless steel overlayer onto an elongate cylindrical substrate comprising:
- securing the substrate horizontally in a fixture adapted to rotate the substrate about a horizontal axis thereof, the substrate having a circumference comprising a bottom arcuate segment, two side arcuate segments, and a top arcuate segment directly opposite and above the bottom arcuate segment;
- maintaining an electrode comprising at least one wire above said top arcuate segment of said substrate while feeding flux onto said top arcuate segment;
- applying a total current to said electrode sufficient to maintain a molten slag pool by ohmic heating of said flux to deposit said overlayer onto the top arcuate segment of said substrate;
- rotating said substrate about said horizontal axis to continually present fresh substrate to said electrode;
- and
- oscillating said electrode at a rate between about 20 and about 40 cycles per minute;
- wherein said electrode contains Ni and Cr and said overlayer comprises at least a first layer in contact with the substrate, wherein dilution of Ni and Cr in said first layer is less than about 25%.
A method for depositing a high alloy stainless steel overlayer onto a roll comprising:
- securing the roll horizontally in a fixture adapted to rotate the substrate about a horizontal axis thereof, the roll having a circumference comprising a bottom arcuate segment, two side arcuate segments, and a top arcuate segment directly opposite and above the bottom arcuate segment;
- maintaining an electrode comprising between one and six filled-core wires containing Ni and Cr above said top arcuate segment of said roll while feeding flux onto said top arcuate segment;
- oscillating said electrode at a rate of between about 20 cycles per minute and about 40 cycles per minute;
- applying a total current to said electrode sufficient to create a molten metal pool and a molten slag pool and maintain said molten slag pool by ohmic heating of said flux to deposit said overlayer onto the top arcuate segment of said roll;
- and
- rotating said substrate about said horizontal axis to continually present fresh substrate to said electrode;
- wherein dilution of Ni and Cr in said overlayer is less than about 25%.
A method for depositing a high alloy stainless steel overlayer onto an elongate cylindrical steel mill roll comprising:
- securing the steel mill roll horizontally in a fixture adapted to rotate the steel mill roll about a horizontal axis thereof, the steel mill roll having circumference comprising a bottom arcuate segment, two side arcuate segments, and a top arcuate segment directly opposite and above the bottom arcuate segment;
- oscillating two filled-core Ni-containing and Cr-containing wire electrodes spaced apart between about 6 mm and about 25 mm at a rate of between about 20 cycles per minute and about 40 cycles per minute with an oscillation path width of between about 13 mm and about 25 mm per electrode while maintaining said electrodes above said top arcuate segment of said roll a distance of between about 25 mm and about 50 mm;
- feeding flux onto said top arcuate segment of said roll around said electrodes by a vibrating flux feeder;
- applying a total current to said electrodes of between about 300 and about 1200 amps to deposit said overlayer onto said top arcuate segment within a molten slag pool maintained by ohmic heating of said flux, wherein dilution of Ni and Cr in said deposit is maintain below about 25%;
- rotating said steel mill roll about its horizontal axis at a speed of between about 100 mm and about 250 mm per minute to continually present fresh roll to said electrodes;
- holding a stainless steel brush against said roll at a position in front of said electrodes such that the roll is rotated under said brush prior to traveling under said electrodes to prevent molten slag from rolling off the roll;
- and
- applying a vacuum pick up at a distance above said molten slag pool to remove excess flux and to increase air flow above the molten slag pool thereby increasing a rate at which said slag pool solidifies.
Dependencies are inferred from the claim text.