A method of joining similar or dissimilar ceramic and ceramic composite materials, such as SiC continuous fiber ceramic composites, at relatively low joining temperatures uses a solventless, three component bonding agent effective to promote mechanical bond toughness and elevated temperature strength to operating temperatures of approximately 1200 degrees C. The bonding agent comprises a preceramic precursor, an aluminum bearing powder, such as aluminum alloy powder, and mixtures of aluminum metal or alloy powders with another powder, and and boron powder in selected proportions. The bonding agent is disposed as an interlayer between similar or dissimilar ceramic or cermaic composite materials to be joined and is heated in ambient air or inert atmosphere to a temperature not exceeding about 1200 degrees C. to form a strong and tough bond joint between the materials. The bond joint produced is characterized by a composite joint microstructure having relatively soft, compliant aluminum bearing particulate regions dispersed in a ceramic matrix.
A method of joining ceramic or ceramic composite materials, comprising disposing a bonding agent at an interface between said materials wherein the bonding agent comprises a preceramic polymer, aluminum bearing particulates, and boron particulates in proportions effective to form upon heating a joint comprising metallic phase regions comprising aluminum disposed in a ceramic joint material and heating the interface to a temperature not exceeding about 1200 degrees C. to form said joint between the materials.
A method of repairing ceramic or ceramic composite material, comprising filling a crack, hole or depression in the material with a bonding agent comprising a preceramic polymer, aluminum bearing particulates, and boron particulates in proportions effective to form upon heating a filler comprising metallic phase regions comprising aluminum disposed in a ceramic filler material and heating the bonding agent to a temperature not exceeding about 1200 degrees C. to form said filler in said crack, hole or depression.
A method of joining ceramic or ceramic composite materials, comprising disposing a bonding agent at an interface between said materials wherein the bonding agent comprises a preceramic polymer, aluminum bearing particulates, and boron particulates in proportions effective to form upon heating a joint comprising metallic phase regions comprising aluminum disposed in a ceramic joint material and heating the interface in an oxygen bearing atmosphere to a temperature not exceeding about 1200 degrees C. to form said joint between the materials.
A method of repairing ceramic or ceramic composite material, comprising filling a crack, hole or depression in the material with a bonding agent comprising a preceramic polymer, aluminum bearing particulates, and boron particulates in proportions effective to form upon heating a filler comprising metallic phase regions comprising aluminum disposed in a ceramic filler material and heating the bonding agent in an oxygen bearing atmosphere to a temperature not exceeding about 1200 degrees C. to form said filler in the crack, hole or depression.
Dependencies are inferred from the claim text.