Abstract
A method of making ferroelectric thin film composites includes the step of roviding a barium strontium titanate material with an additive magnesia-based and forming a thin film ferroelectric composite using pulsed laser deposition. The method forms a thin film composite having enhanced electronic properties.
Claims10
A method of making a thin film of a ferroelectric composite material having a composition comprising:
- barium strontium titanate, said barium strontium titanate represented as Ba.sub.1-x Sr.sub.x TiO.sub.3, wherein x is greater than 0.0 but less than or equal to 0.75, and an additive selected from the group consisting of mangesia, alumina, silica, a low dielectric oxide, zirconia, and combinations thereof;
- wherein said barium strontium titanate and said additive are present in effective amounts to provide a composite having a low dielectric constant, low loss tangibles, and high tunability.
- the method comprising the steps of:
- a) providing at least one ceramic disc of said composition as an abalation target;
- b) providing a substrate at a temperature of between 400-700 degrees centigrade, and at a distance between the substrate and target of 25-50 mm;
- c) depositing a thin file of said composition on said substrate using a krypton exciminer pulsed laser utilizing a laser wavelength of 193-248 nm, a laser pulse energy of 226-350 m/J pulse, a pulse width of 10-20 ns and a pulse repetition rate of 5-25 Hz.