Thermosensitive stencil paper and the method of producing the same
AssigneesRicoh Company, Ltd., Tohoku Ricoh Co., Ltd.
InventorsManabu Fujimura, Fumiaki Arai, Hideyuki Yamaguchi, Masayuki Ohta
Life of this patent
Estimating the term…
Loading patent…
AssigneesRicoh Company, Ltd., Tohoku Ricoh Co., Ltd.
InventorsManabu Fujimura, Fumiaki Arai, Hideyuki Yamaguchi, Masayuki Ohta
Estimating the term…
A thermosensitive stencil paper includes a thermoplastic resin film, and optionally a porous support for supporting the resin film thereon, and a silicone oil containing layer formed the resin film, which contains at least one modified silicone oil component selected from the group consisting of (a) an ether.cndot.epoxy-modified silicone oil having both an epoxy group and an ether group and (b) an ether-modified silicone oil with HLB of 6 or less. The above thermosensitive stencil paper can be produced by coating a coating liquid which contains at least one of the above-mentioned modified silicone oils in an amount of 2.0 g/m.sup.2 or less before the drying of the coating liquid.
A thermosensitive stencil paper comprising a thermoplastic resin film, and a modified silicone oil containing layer formed thereon which comprises at least one modified silicone oil component selected from group consisting of (a) an ether.cndot.epoxy-modified silicone oil having both an epoxy group and an ether group and (b) an ether-modified silicone oil with HLB of 6 or less.
A method of producing a thermosensitive stencil paper comprising a thermoplastic resin film, and a modified silicone oil containing layer formed thereon which comprises at least one modified silicone oil component selected from the group consisting of (a) an ether.cndot.epoxy-modified silicone oil having both an epoxy group and an ether group and (a) an ether modified silicone oil with HLB of 6 or less, comprising the step of coating said thermoplastic resin film with a coating liquid comprising at least one modified silicone oil component selected from the group consisting of (a) an ether.cndot.epoxy-modified silicone oil having both an epoxy group and an ether group and (b) an ether-modified silicone oil with HLB of 6 or less, in an amount of 2.0 g/m.sup.2 or less before the drying of said coating liquid.