A method for preparing an amorphous ternary lithiated vanadium metal oxide of the formula Li.sub.x M.sub.y V.sub.z O.sub.(x+5z+ny)/2, where M is a metal, 0<x.ltoreq.3, 0<y.ltoreq.3, 1.ltoreq.z.ltoreq.4, and n=2 or 3
- characterized in that
- a) an aqueous solution is prepared of
- 1) at least one metavanadate salt selected from the group consisting of NH.sub.4 VO.sub.3 and NaVO.sub.3,
- 2) a nitrate salt of the formula M(NO.sub.3).sub.n, where M is said metal, and
- 3) an excess of a lithium salt;
- b) the resulting solution is heated;
- and
- c) a sufficient amount of a base is added to the heated solution to obtain a pH suitable for precipitating the amorphous lithiated vanadium metal oxide.