Unusually high loading levels of smectite minerals are found to provide excellent pigment spacing in aqueous-based coatings, as will enable desired improved hiding, thereby extending the pigment. The level of smectite used in accordance with the invention is sufficiently high that the high gelling efficiency smectites previously used as thixotropes would be inappropriate, and would yield viscosities so high as to render the aqueous coating composition lacking in desired flowability properties. Thus in accordance with the present invention, there is mixed with the aqueous carrier and pigment at least 0.5% by weight of the total composition, of a particulate water swellable smectite which has a gelling efficiency such as to display a 20 rpm Brookfield viscosity of less than 900 cps when subjected to the standard gelling test herein, with the amount of the smectite in the composition not exceeding that which would raise the viscosity of the composition above 110 Krebs Units (KU).
A method for extending the ability of a pigment which is suspended in an aqueous carrier of a coating composition, to obscure an underlying surface upon which said composition has dried to a film, comprising:
An aqueous pigment-containing composition having high hiding power to obscure a surface when the composition is applied on said surface and dried to a film;
Dependencies are inferred from the claim text.