Ceramic coating system or water oxidation environments
AssigneeModar, Inc.
InventorGlenn T. Hong
Life of this patent
Estimating the term…
Loading patent…
AssigneeModar, Inc.
InventorGlenn T. Hong
Estimating the term…
A process for water oxidation of combustible materials in which during at least a part of the oxidation corrosive material is present and makes contact with at least a portion of the apparatus over a contact area on the apparatus. At least a portion of the contact surface area comprises titanium dioxide coated onto a titanium metal substrate. Such ceramic composites have been found to be highly resistant to environments encountered in the process of supercritical water oxidation. Such environments typically contain greater than 50 mole percent water, together with oxygen, carbon dioxide, and a wide range of acids, bases, and salts. Pressures are typically about 27.5 to about 1000 bar while temperatures range as high as 700.degree. C. The ceramic composites are also resistant to degradation mechanisms caused by thermal stresses.
A process for high temperature water oxidation of combustible material in a high temperature water oxidation apparatus, in which during at least part of the oxidation, corrosive material is present and contacts the apparatus over a contact area on the apparatus, the process comprising contacting in an aqueous phase the combustible material and an oxidizing agent under conditions suitable to cause oxidation of the combustible material, wherein the oxidation is at a temperature in the range of about 300.degree. C. to about 700.degree. C. and at pressures from about 27.5 bar (400 psi) to about 1000 bar (15,000 psi) and the contact area contains a ceramic composite comprising titanium base metal overlaid with a titania coating, to provide corrosion resistance from said corrosive material in said contact area.
A process of oxidizing combustible materials containing corrosive constituents in an oxidation apparatus in which an aqueous phase containing the oxidizable combustible material and oxidizing agent is contacted with at least a portion of a contact area of the apparatus under conditions suitable to cause oxidation of the combustible material, at a temperature of at least about 300.degree. C. and a pressure of at least about 27.5 bar, wherein said corrosive constituents are present in said contact area, and wherein the contact area contains a ceramic composite consisting of titanium dioxide coated onto a titanium metal substrate to provide corrosion resistance from said corrosive constituents in said contact area.
A process for oxidizing combustible material in a water oxidation apparatus, in which during at least part of the oxidation, corrosive material is present and contacts the apparatus over a contact area on the apparatus, the process comprising contacting in an aqueous phase the combustible material and an oxidizing agent under conditions suitable to cause oxidation of the combustible material at a temperature of at least about 300.degree. C. and a pressure of at least about 27.5 bar, wherein the contact area contains a ceramic composite comprising titanium base metal overlaid with a titania coating, to provide corrosion resistance from said corrosive material in said contact area.
Dependencies are inferred from the claim text.